  Technyl® C 502XT | PA6 | Rhodia Polyamide Engineering Plastics
제품 설명서
Unreinforced polyamide 6, very high viscosity, for extrusion.
기계적 특성건조/응축단위시험규격
인장탄성률 2800 / 900 MPa ISO 527-1/-2
항복강도 80 / - MPa ISO 527-1/-2
항복변형률 4.1 / - % ISO 527-1/-2
파단시 평균신율 >50 / - % ISO 527-1/-2
챠피 충격 강도 , +23°C N / - kJ/m² ISO 179/1eU
열적 특성건조/응축단위시험규격
녹는점, 10°C/min 222 / * °C ISO 11357-1/-3
기타 특성건조/응축단위시험규격
조건에서의 흡습성 1.37 / * % ISO 62와 유사
밀도 1130 / - kg/m³ ISO 1183
도표
응력-신율 , Technyl® C 502XT, PA6, Rhodia
Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012