Ultramid® 8266G HS BK102 | PA6-(MD+GF)40 | BASF
제품 설명서
Ultramid® 8266G HS is a heat stabilized, 40% mineral and glass, injection molding compound. It possesses a balance of engineering properties in combination with excellent dimensional stability, low warp and resistance to sink-mark formation. It is also available in non-heat stabilized (Ultramid® 8266G) and/or pigmented versions.
Ultramid® 8266G HS is generally recommended for high performance applications such as painted automotive housings and exterior body parts, brackets, wheel hubs, shrouds, roller bearings, and push-pull cable components.
Ultramid® 8266G HS is generally recommended for high performance applications such as painted automotive housings and exterior body parts, brackets, wheel hubs, shrouds, roller bearings, and push-pull cable components.
| 기계적 특성 | 건조/응축 | 단위 | 시험규격 |
| 인장탄성률 | 9780 / 5610 | MPa | ISO 527-1/-2 |
| 파단시 강도 | 125 / 70 | MPa | ISO 527-1/-2 |
| 파단시 신율 | 3 / 6 | % | ISO 527-1/-2 |
| 챠피 노치드 충격 강도, +23°C | 4 / - | kJ/m² | ISO 179/1eA |
| 열적 특성 | 건조/응축 | 단위 | 시험규격 |
| 녹는점, 10°C/min | 220 / * | °C | ISO 11357-1/-3 |
| 하중하에서의 변형온도, 1.80 MPa | 205 / * | °C | ISO 75-1/-2 |
| 하중하에서의 변형온도, 0.45 MPa | 217 / * | °C | ISO 75-1/-2 |
| 선형 열팽창 계수, 평행 | 21 / * | E-6/K | ISO 11359-1/-2 |
| 선형 열팽창 계수, 수직 | 58 / * | E-6/K | ISO 11359-1/-2 |
| 두께 H인 제품의 난연성 | HB / * | class | IEC 60695-11-10 |
| 테스트 두께 | 3.0 / * | mm | IEC 60695-11-10 |
| UL 승인품의 난연성 | UL / * | - | - |
| 전기적 특성 | 건조/응축 | 단위 | 시험규격 |
| 부피 저항 | >1E13 / - | Ohm*m | IEC 60093 |
| 테스트 견본 생산 | 값 | 단위 | 시험규격 |
| 사출성형: 용융수지온도 | 275 | °C | ISO 294 |
| 사출성형: 금형온도 | 95 | °C | ISO 10724 |
도표
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
열안정성
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact your local BASF
representative or
BASF SE
Dept. PM/K
Fax: 0621-60-49497
e-mail: e-mail
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact your local BASF
representative or
BASF SE
Dept. PM/K
Fax: 0621-60-49497
e-mail: e-mail
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012