CAMPUSplastics | All PBT grades

The international CAMPUS® database offers datasheets of the following grades that are related to the polymer family: PBT.

Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.

Grade Name Family Producer
ALCOM® PBT 700/1 GF20 PTFE15 (PBT+PTFE)-GF20 ALBIS Plastic GmbH
ALCOM® PBT 700/1 GF30 PTFE15 (PBT+PTFE)-GF30 ALBIS Plastic GmbH
ALCOM® PBT 700/1 GF30 PTFE15 Si2 (PBT+PTFE)-GF... ALBIS Plastic GmbH
ALCOM® PBT 700/1 PTFE20 (PBT+PTFE) ALBIS Plastic GmbH
ALCOM® PBT 700/1.1 CF20 PTFE15 (PBT+PTFE)-CF ALBIS Plastic GmbH
ALCOM® PBT 700/1.5 GF15 PTFE15 (PBT+PTFE)-GF15 ALBIS Plastic GmbH
ALCOM® PBT 700/1.5 GF15 PTFE15 HR (PBT+PTFE)-GF15 ALBIS Plastic GmbH
ALCOM® PBT 700/2 WT 31-956 LB PBT ALBIS Plastic GmbH
ALCOM® PBT 700/30.1 TCE10 PBT... ALBIS Plastic GmbH
ALCOM® PBT 700/30.2 TCD2 PBT... ALBIS Plastic GmbH
ALCOM® PBT 700/8 GF15 PTFE15 (PBT+PTFE)-GF15 ALBIS Plastic GmbH
ALTECH PBT A 1000/506 PBT ALBIS Plastic GmbH
ALTECH PBT A 1000/507 PBT ALBIS Plastic GmbH
ALTECH PBT A 2020/340 GF20 FR PBT-GF20 FR ALBIS Plastic GmbH
ALTECH PBT A 2020/510 GF20 IM PBT-I-GF20 ALBIS Plastic GmbH
ALTECH PBT A 2030/340 GF30 FR PBT-GF30 FR ALBIS Plastic GmbH
ALTECH PBT A 3030/100 GB30 PBT-GB30 ALBIS Plastic GmbH
ALTECH PBT+ASA A 2020/510 GF20 (PBT+ASA)-GF20 ALBIS Plastic GmbH
ALTECH PBT+ASA A 2030/500 GF30 (PBT+ASA)-GF30 ALBIS Plastic GmbH
Arnite® B434 SE PBT-GF20 FR(17) DSM Engineering Plastics
Arnite® B436 SE PBT-GF30 FR(17) DSM Engineering Plastics
Arnite® B437 SE/R PBT-GF35 FR(17) DSM Engineering Plastics
Arnite® B600 SNF PBT FR DSM Engineering Plastics
Arnite® B600SE PBT FR DSM Engineering Plastics
Arnite® B604T PBT-I DSM Engineering Plastics
Arnite® BM4 240 (PBT+PET)-MD20 DSM Engineering Plastics
Arnite® T04 200 PBT DSM Engineering Plastics
Arnite® T06 200 PBT DSM Engineering Plastics
Arnite® T06 200 (extrusion) PBT DSM Engineering Plastics
Arnite® T06 200 /D PBT DSM Engineering Plastics
Arnite® T06 202 PBT DSM Engineering Plastics
Arnite® T06 202 /A PBT DSM Engineering Plastics
Arnite® T06 202 XL PBT DSM Engineering Plastics
Arnite® T06 204 SN PBT FR(17) DSM Engineering Plastics
Arnite® T06 204 XL PBT DSM Engineering Plastics
Arnite® T08 200 PBT DSM Engineering Plastics
Arnite® T08 200 (extrusion) PBT DSM Engineering Plastics
Arnite® TB6 260 PBT-GB30 DSM Engineering Plastics
Arnite® TM4 440 (PBT+PET)-MD20 DSM Engineering Plastics
Arnite® TV4 220 PBT-GF10 DSM Engineering Plastics
Arnite® TV4 230 PBT-GF15 DSM Engineering Plastics
Arnite® TV4 230 S PBT-GF15 FR(17) DSM Engineering Plastics
Arnite® TV4 230 SF PBT-GF15 FR(17) DSM Engineering Plastics
Arnite® TV4 240 PBT-GF20 DSM Engineering Plastics
Arnite® TV4 240 S PBT-GF20 FR(17) DSM Engineering Plastics
Arnite® TV4 241 SL PBT-GF20 FR(17) DSM Engineering Plastics
Arnite® TV4 241 SN PBT-GF20 FR(17) DSM Engineering Plastics
Arnite® TV4 244 S PBT-GF20 FR DSM Engineering Plastics
Arnite® TV4 244 SX PBT-GF20 FR(17) DSM Engineering Plastics
Arnite® TV4 260 S PBT-GF30 FR(17) DSM Engineering Plastics
Arnite® TV4 260 SN PBT-GF30 FR(17) DSM Engineering Plastics
Arnite® TV4 260 SXF PBT-GF30 FR(17) DSM Engineering Plastics
Arnite® TV4 261 PBT-GF30 DSM Engineering Plastics
Arnite® TV4 261 KL PBT-GF30 DSM Engineering Plastics
Arnite® TV4 261 SF PBT-GF30 FR(17) DSM Engineering Plastics
Arnite® TV4 264 SN PBT-GF30 FR(17) DSM Engineering Plastics
Arnite® TV4 270 PBT-GF35 DSM Engineering Plastics
Arnite® TV4 290 PBT-GF50 DSM Engineering Plastics
Arnite® TV4 441 (PBT+PET)-GF20 DSM Engineering Plastics
Arnite® TV4 460 KL (PBT+PET)-GF30 DSM Engineering Plastics
Arnite® TV4 461 (PBT+PET)-GF30 DSM Engineering Plastics
Arnite® TV4 461 KL (PBT+PET)-GF30 DSM Engineering Plastics
Arnite® TV4 491 (PBT+PET)-GF50 DSM Engineering Plastics
Arnite® TV4 640 (PBT+PC)-GF20 DSM Engineering Plastics
Arnite® TV4 660 SN (PBT+PC)-GF30 FR DSM Engineering Plastics
Arnite® TV6 220 PBT-GF10 DSM Engineering Plastics
Arnite® TV6 240 PBT-GF20 DSM Engineering Plastics
Arnite® TV6 241 SN PBT-GF20 FR(17) DSM Engineering Plastics
Arnite® TV6 241 T PBT-I-GF20 DSM Engineering Plastics
Arnite® TV6 260 T PBT-I-GF30 DSM Engineering Plastics
Arnite® TV8 260 PBT-GF30 DSM Engineering Plastics
Arnite® TZ4 254 S PBT-(GF+MD)25 FR(17) DSM Engineering Plastics
Arnite® TZ6 280 PBT-(GF+GB)40 DSM Engineering Plastics
Arnite® TZ6 280 BLK ( NCP-4718/B ) PBT-(GF+GB)40 DSM Engineering Plastics
Arnite® XG 260 S (T-X07086) PBT-GF30 FR DSM Engineering Plastics
BERGADUR® PB40/50 PBT PolyOne Engineered Materials Europe
BERGADUR® PB400G/MI35UBK PBT-(GF+MD)35 PolyOne Engineered Materials Europe
BERGADUR® PB400G/MI45U PBT-(GF+MD)45 PolyOne Engineered Materials Europe
BERGADUR® PB400G30U PBT-GF30 PolyOne Engineered Materials Europe
BERGADUR® PB400G7,5UNATUR PBT-GF7 PolyOne Engineered Materials Europe
BERGADUR® PB40G/GK30 PBT-(GF+GB)30 PolyOne Engineered Materials Europe
BERGADUR® PB40G10 PBT-GF10 PolyOne Engineered Materials Europe
BERGADUR® PB40G20 PBT-GF20 PolyOne Engineered Materials Europe
BERGADUR® PB40G20U PBT-GF20 PolyOne Engineered Materials Europe
BERGADUR® PB40G30 PBT-GF30 PolyOne Engineered Materials Europe
BERGADUR® PB40G30TM-Z PBT-GF30 PolyOne Engineered Materials Europe
BERGADUR® PB40G30UM PBT-GF20 PolyOne Engineered Materials Europe
BERGADUR® PB40G40 PBT-GF40 PolyOne Engineered Materials Europe
BERGADUR® PB40GK30 PBT-GB30 PolyOne Engineered Materials Europe
BERGADUR® PB40GK30U PBT-GB30 PolyOne Engineered Materials Europe
BERGADUR® PB40TM-Y PBT PolyOne Engineered Materials Europe
BERGADUR® PB40TM-Z PBT PolyOne Engineered Materials Europe
BERGADUR® PB40UM PBT PolyOne Engineered Materials Europe
BERGADUR® PB450UA PBT PolyOne Engineered Materials Europe
BERGADUR® PB450UB PBT PolyOne Engineered Materials Europe
CELANEX 1400A PBT Ticona
CELANEX 1462Z PBT-GF30 Ticona
CELANEX 1600A PBT Ticona
CELANEX 1602Z PBT Ticona
CELANEX 1632Z PBT-GF15 Ticona
CELANEX 1642Z PBT-GF20 Ticona
CELANEX 1662Z PBT-GF30 Ticona
CELANEX 1700A PBT Ticona
CELANEX 2000-2 PBT Ticona
CELANEX 2000-3 PBT Ticona
CELANEX 2001 PBT Ticona
CELANEX 2002-2 PBT Ticona
CELANEX 2002-3 PBT Ticona
CELANEX 2002UV PBT Ticona
CELANEX 2003-2 PBT Ticona
CELANEX 2003-3 PBT Ticona
CELANEX 2003HR PBT Ticona
CELANEX 2004-2 PBT Ticona
CELANEX 2008 PBT Ticona
CELANEX 2016 PBT Ticona
CELANEX 2300 GV1/10 PBT-GF10 Ticona
CELANEX 2300 GV1/20 PBT-GF20 Ticona
CELANEX 2300 GV1/30 PBT-GF30 Ticona
CELANEX 2300 GV1/50 PBT-GF50 Ticona
CELANEX 2300 GV3/20 PBT-GB20 Ticona
CELANEX 2300 GV3/30 PBT-GB30 Ticona
CELANEX 2302 GV1/15 PBT-GF15 Ticona
CELANEX 2302 GV1/20 PBT-GF20 Ticona
CELANEX 2302 GV1/30 PBT-GF30 Ticona
CELANEX 2401 MT PBT Ticona
CELANEX 2402 MT PBT Ticona
CELANEX 2404 MT PBT Ticona
CELANEX 2500 PBT Ticona
CELANEX 3100-2 PBT-GF7 Ticona
CELANEX 3105H PBT-GF15 Ticona
CELANEX 3109HR PBT-GF7 Ticona
CELANEX 3116 PBT-GF7 Ticona
CELANEX 3200 PBT-GF15 Ticona
CELANEX 3200-2 PBT-GF15 Ticona
CELANEX 3200HR PBT-GF15 Ticona
CELANEX 3201 PBT-GF15 Ticona
CELANEX 3202-2 PBT Ticona
CELANEX 3209HR PBT Ticona
CELANEX 3209HRT PBT-GF15 Ticona
CELANEX 3216 PBT-GF15 Ticona
CELANEX 3225HRT PBT-GF15 Ticona
CELANEX 3226 PBT Ticona
CELANEX 3300 PBT-GF30 Ticona
CELANEX 3300-2 PBT-GF30 Ticona
CELANEX 3300-2LM PBT Ticona
CELANEX 3300D PBT-GF30 Ticona
CELANEX 3300HR PBT-GF30 Ticona
CELANEX 3300LM PBT-GF30 Ticona
CELANEX 3309HR PBT-GF30 Ticona
CELANEX 3309HRHF PBT-GF30 Ticona
CELANEX 3309HRLM PBT-GF30 Ticona
CELANEX 3309HRT PBT-GF30 Ticona
CELANEX 3316 PBT-GF30 Ticona
CELANEX 3316CT PBT-(GF+MD)50 Ticona
CELANEX 3318 PBT-GF30 Ticona
CELANEX 3325HRT PBT-GF30 Ticona
CELANEX 3400-2 PBT-GF40 Ticona
CELANEX 3409HR PBT-GF40 Ticona
CELANEX 3425HRT PBT Ticona
CELANEX 4016 PBT Ticona
CELANEX 4022 PBT Ticona
CELANEX 4202 PBT-GF15 Ticona
CELANEX 4300 PBT-GF30 Ticona
CELANEX 4300LM PBT-GF30 Ticona
CELANEX 4302 PBT-GF30 Ticona
CELANEX 4302HS PBT-GF30 Ticona
CELANEX 4302LM PBT-GF30 Ticona
CELANEX 4305 PBT-GF33 Ticona
CELANEX 4306 PBT-GF30 Ticona
CELANEX 5200-2 PBT-GF15 Ticona
CELANEX 5202 PBT-GF15 Ticona
CELANEX 5202HF PBT-GF15 Ticona
CELANEX 5205HG PBT-GF15 Ticona
CELANEX 5214HF PBT-GF15 Ticona
CELANEX 5300-2 PBT-GF30 Ticona
CELANEX 5300-2UV PBT-GF30 Ticona
CELANEX 531HS PBT Ticona
CELANEX 602AC PBT Ticona
CELANEX 6035GB20 PBT-GB20 Ticona
CELANEX 6400-2 PBT Ticona
CELANEX 6402R PBT-(GF+MX)40 Ticona
CELANEX 6406 PBT-(GF+P)40 Ticona
CELANEX 6407 PBT-(GF+P)30 Ticona
CELANEX 6407HR PBT-(GF+P)30 Ticona
CELANEX 6500 PBT-(GF+P)30 Ticona
CELANEX 6500HF PBT Ticona
CELANEX 6500HR PBT Ticona
CELANEX 6500LM PBT-(GF+P)30 Ticona
CELANEX 7316 PBT-(GF+P)35 Ticona
CELANEX 733LD PBT Ticona
CELANEX 7407 PBT-GF40 Ticona
CELANEX 7714 PBT Ticona
CELANEX 7716 PBT-(GF+P)35 Ticona
CELANEX D3200LC PBT Ticona
CELANEX J235 PBT Ticona
CELANEX J600 PBT-(GF+P)40 Ticona
CELANEX LW2333R PBT-(GB+GF)50 Ticona
CELANEX LW2547W PBT-(GF+MX)30 Ticona
CELANEX XFR 4840 PBT Ticona
CELANEX XFR 4840 10/0242 Black PBT Ticona
CELANEX XFR 6842 GF10 PBT-GF30 Ticona
CELANEX XFR 6842 GF15 PBT-GF30 Ticona
CELANEX XFR 6842 GF20 PBT-GF30 Ticona
CELANEX XFR 6842 GF30 PBT-GF30 Ticona
CELSTRAN PBT-CF40-08 PBT-CF40 Ticona
CELSTRAN PBT-GF30-08 PBT-GF30 Ticona
CELSTRAN PBT-GF40-08 PBT-GF40 Ticona
CELSTRAN PBT-GF50-08 PBT-GF50 Ticona
Crastin® 6129 NC010 PBT DuPont Engineering Polymers
Crastin® 6130 NC010 PBT DuPont Engineering Polymers
Crastin® 6131 NC010 PBT DuPont Engineering Polymers
Crastin® 6134 NC010 PBT DuPont Engineering Polymers
Crastin® BM6450XD BK560 PBT DuPont Engineering Polymers
Crastin® CE15315 NC010 PBT-GF15 FR(17) DuPont Engineering Polymers
Crastin® CE15330 NC010 PBT-GF30 FR(17) DuPont Engineering Polymers
Crastin® CE2055 NC010 PBT DuPont Engineering Polymers
Crastin® CE2255 BK580 PBT DuPont Engineering Polymers
Crastin® FG6129 NC010 PBT DuPont Engineering Polymers
Crastin® FG6130 NC010 PBT DuPont Engineering Polymers
Crastin® FGS600F40 NC010 PBT DuPont Engineering Polymers
Crastin® FR1000TC BK350 PBT FR DuPont Engineering Polymers
Crastin® FR1100TC BK350 PBT FR DuPont Engineering Polymers
Crastin® HR5315HF NC010 PBT-I-GF15 DuPont Engineering Polymers
Crastin® HR5315HFS NC010 PBT-I-GF15 DuPont Engineering Polymers
Crastin® HR5330HF NC010 PBT-I-GF30 DuPont Engineering Polymers
Crastin® HR5330HFS NC010 PBT-I-GF30 DuPont Engineering Polymers
Crastin® LW9020 NC010 (PBT+ASA)-GF20 DuPont Engineering Polymers
Crastin® LW9020FR NC010 (PBT+ASA)-GF20 FR(17) DuPont Engineering Polymers
Crastin® LW9030 NC010 (PBT+ASA)-GF30 DuPont Engineering Polymers
Crastin® LW9030FR NC010 (PBT+ASA)-GF30 FR(17) DuPont Engineering Polymers
Crastin® LW9320 NC010 (PBT+SAN)-I-GF20 DuPont Engineering Polymers
Crastin® LW9320LM BK591 (PBT+SAN)-I-GF20 DuPont Engineering Polymers
Crastin® LW9330 NC010 (PBT+SAN)-I-GF30 DuPont Engineering Polymers
Crastin® S600F10 NC010 PBT DuPont Engineering Polymers
Crastin® S600F20 NC010 PBT DuPont Engineering Polymers
Crastin® S600F40 NC010 PBT DuPont Engineering Polymers
Crastin® S610SF NC010 PBT DuPont Engineering Polymers
Crastin® S620F20 NC010 PBT DuPont Engineering Polymers
Crastin® S650FR NC010 PBT FR(17) DuPont Engineering Polymers
Crastin® SC164 NC010 PBT DuPont Engineering Polymers
Crastin® SC193 NC010 (PBT+ASA)-GF30 DuPont Engineering Polymers
Crastin® SK601 NC010 PBT-GF10 DuPont Engineering Polymers
Crastin® SK602 NC010 PBT-GF15 DuPont Engineering Polymers
Crastin® SK603 NC010 PBT-GF20 DuPont Engineering Polymers
Crastin® SK605 NC010 PBT-GF30 DuPont Engineering Polymers
Crastin® SK608 BK509 PBT-GF45 DuPont Engineering Polymers
Crastin® SK609 NC010 PBT-GF50 DuPont Engineering Polymers
Crastin® SK612SF NC010 PBT-GF15 DuPont Engineering Polymers
Crastin® SK615SF NC010 PBT-GF30 DuPont Engineering Polymers
Crastin® SK641FR NC010 PBT-GF10 FR(17) DuPont Engineering Polymers
Crastin® SK642FR NC010 PBT-GF15 FR(17) DuPont Engineering Polymers
Crastin® SK643FR NC010 PBT-GF20 FR(17) DuPont Engineering Polymers
Crastin® SK645FR NC010 PBT-GF30 FR(17) DuPont Engineering Polymers
Crastin® SO653 NC010 PBT-GB20 DuPont Engineering Polymers
Crastin® ST820 NC010 PBT-I DuPont Engineering Polymers
Crastin® ST830FRUV NC010 PBT-I FR(17) DuPont Engineering Polymers
Hytrel® DYM250S BK472 (TPC+PBT) DuPont Engineering Polymers
Hytrel® DYM350BK (TPC+PBT) DuPont Engineering Polymers
Makroblend® KU2-7609 (PC+PBT)-I-MD20 Bayer MaterialScience
Makroblend® KU2-7912/4 (PC+PBT)-I Bayer MaterialScience
Makroblend® KU2-7915 (PC+PBT)-I Bayer MaterialScience
Makroblend® S7916 (PBT+PC)-I Bayer MaterialScience
Makroblend® UT1018 (PC+PBT) Bayer MaterialScience
Makroblend® UT3905 (PC+PBT)-I Bayer MaterialScience
Makroblend® UT3907 (PC+PBT)-I Bayer MaterialScience
Makroblend® UT4045 G (PC+PBT)-GF20 Bayer MaterialScience
Makroblend® UT408 (PC+PBT) Bayer MaterialScience
Makroblend® UT6005 (PC+PBT)-I Bayer MaterialScience
Makroblend® UT6007 (PC+PBT)-I Bayer MaterialScience
Pocan® A 3131 (PBT+ASA)-GF30 LANXESS Deutschland GmbH
Pocan® B 1100 PBT LANXESS Deutschland GmbH
Pocan® B 1300 PBT LANXESS Deutschland GmbH
Pocan® B 1305 PBT LANXESS Deutschland GmbH
Pocan® B 1501 PBT LANXESS Deutschland GmbH
Pocan® B 1505 PBT LANXESS Deutschland GmbH
Pocan® B 1505 Z PBT LANXESS Deutschland GmbH
Pocan® B 1600 PBT LANXESS Deutschland GmbH
Pocan® B 1700 PBT LANXESS Deutschland GmbH
Pocan® B 1701 PBT LANXESS Deutschland GmbH
Pocan® B 2505 PBT FR LANXESS Deutschland GmbH
Pocan® B 3215 PBT-GF10 LANXESS Deutschland GmbH
Pocan® B 3215 XF PBT-I-GF10 LANXESS Deutschland GmbH
Pocan® B 3215 Z PBT-GF10 LANXESS Deutschland GmbH
Pocan® B 3217 XF PBT-I-GF16 LANXESS Deutschland GmbH
Pocan® B 3225 PBT-GF20 LANXESS Deutschland GmbH
Pocan® B 3225 XF PBT-GF20 LANXESS Deutschland GmbH
Pocan® B 3225 Z PBT-GF20 LANXESS Deutschland GmbH
Pocan® B 3233 HR PBT-GF30 LANXESS Deutschland GmbH
Pocan® B 3235 PBT-GF30 LANXESS Deutschland GmbH
Pocan® B 3235 XF PBT-GF30 LANXESS Deutschland GmbH
Pocan® B 4215 PBT-GF12 FR LANXESS Deutschland GmbH
Pocan® B 4225 PBT-GF20 FR LANXESS Deutschland GmbH
Pocan® B 4235 PBT-GF30 FR LANXESS Deutschland GmbH
Pocan® B 4235 Z PBT-GF30 FR LANXESS Deutschland GmbH
Pocan® B 4239 PBT-GF30 FR LANXESS Deutschland GmbH
Pocan® B 5220 XF PBT-I-GB20 LANXESS Deutschland GmbH
Pocan® B 700 PBT LANXESS Deutschland GmbH
Pocan® B 7375 PBT-X25 LANXESS Deutschland GmbH
Pocan® B 7425 PBT-GB20 LANXESS Deutschland GmbH
Pocan® B 7616 (PBT+PC)-GF15 LANXESS Deutschland GmbH
Pocan® BF 4130 XF PBT-GF30 FR LANXESS Deutschland GmbH
Pocan® BF 4215 PBT-GF12 FR LANXESS Deutschland GmbH
Pocan® BF 4225 PBT-GF20 FR LANXESS Deutschland GmbH
Pocan® BF 4235 PBT-GF30 FR LANXESS Deutschland GmbH
Pocan® BF 4409 PBT-GF7 FR LANXESS Deutschland GmbH
Pocan® BF 8230 PBT-(GF+GB)30 FR LANXESS Deutschland GmbH
Pocan® C 1202 (PBT+PC)-I LANXESS Deutschland GmbH
Pocan® C 3230 XF (PBT+PC)-GF30 LANXESS Deutschland GmbH
Pocan® DP 1105 PBT LANXESS Deutschland GmbH
Pocan® DP 2004 PBT FR LANXESS Deutschland GmbH
Pocan® DP 4035 (PBT+PET)-GF30 FR LANXESS Deutschland GmbH
Pocan® DP 7102 PBT-MD30 LANXESS Deutschland GmbH
Pocan® DP 7244 PBT-GF30 FR LANXESS Deutschland GmbH
Pocan® DP BF 4232 PBT-GF30 FR LANXESS Deutschland GmbH
Pocan® DP C 1502 (PBT+PC)-I LANXESS Deutschland GmbH
Pocan® DP CF 2200 (PBT+PC) FR LANXESS Deutschland GmbH
Pocan® DP T7140 LDS (PET+PBT)-(MD+GF)44 LANXESS Deutschland GmbH
Pocan® ECO T 3220 (PBT+PET)-GF20 LANXESS Deutschland GmbH
Pocan® ECO T 3230 (PBT+PET)-GF30 LANXESS Deutschland GmbH
Pocan® ECO T 3240 (PBT+PET)-GF45 LANXESS Deutschland GmbH
Pocan® KL 1-7033 PBT-GF30 LANXESS Deutschland GmbH
Pocan® KL 1-7265 PBT-GF15 LANXESS Deutschland GmbH
Pocan® KU 1-7301 PBT LANXESS Deutschland GmbH
Pocan® KU 1-7313 (PBT+PET)-GF15 LANXESS Deutschland GmbH
Pocan® KU 1-7625 (PBT+PC)-GF20 LANXESS Deutschland GmbH
Pocan® KU 1-7635 (PBT+PC)-GF30 LANXESS Deutschland GmbH
Pocan® KU 1-7635 POS151 (PBT+PC)-GF30 LANXESS Deutschland GmbH
Pocan® KU 2-7003 PBT LANXESS Deutschland GmbH
Pocan® KU 2-7018 PBT LANXESS Deutschland GmbH
Pocan® KU 2-7205 PBT FR LANXESS Deutschland GmbH
Pocan® KU 2-7209 Z PBT-GF15 FR LANXESS Deutschland GmbH
Pocan® KU 2-7317 PBT-I-Z17 LANXESS Deutschland GmbH
Pocan® KU 2-7503/1 PBT FR LANXESS Deutschland GmbH
Pocan® KU 2-7604 (PBT+PC) FR LANXESS Deutschland GmbH
Pocan® S 1506 PBT LANXESS Deutschland GmbH
Pocan® S 1517 PBT LANXESS Deutschland GmbH
Pocan® S 7020 PBT FR LANXESS Deutschland GmbH
Pocan® S 7926 PBT FR LANXESS Deutschland GmbH
Pocan® T 3150 XF (PBT+PET)-GF55 LANXESS Deutschland GmbH
Pocan® T 7323 (PBT+PET)-GF20 LANXESS Deutschland GmbH
Pocan® T 7323 POS151 (PBT+PET)-GF20 LANXESS Deutschland GmbH
Pocan® T 7331 (PBT+PET)-GF30 LANXESS Deutschland GmbH
Pocan® T 7331 POS151 (PBT+PET)-GF30 LANXESS Deutschland GmbH
Pocan® T 7391 (PBT+PET)-GF45 LANXESS Deutschland GmbH
Pocan® T 7391 POS151 (PBT+PET)-GF45 LANXESS Deutschland GmbH
Pocan® TS 3220 (PBT+PET)-I-GF20 LANXESS Deutschland GmbH
RADIFLAM® B N100AE PBT FR RadiciPlastics
RADIFLAM® B RV250AE PBT-GF25 FR RadiciPlastics
RADITER® B N100 PBT RadiciPlastics
RADITER® B RV150 PBT-GF15 RadiciPlastics
RADITER® B RV200 PBT-GF20 RadiciPlastics
RADITER® B RV300 PBT-GF30 RadiciPlastics
RADITER® B RVA100 (PBT+ASA)-GF10 RadiciPlastics
RADITER® B RVA200 (PBT+ASA)-GF20 RadiciPlastics
RADITER® B RVA300 (PBT+ASA)-GF30 RadiciPlastics
SCHULABLEND® M/MX 50 (PBT+PC)... A. Schulman GmbH
SCHULADUR® A BS 40 HI PBT-I-Z40 A. Schulman GmbH
SCHULADUR® A GB 20 PBT-GB20 A. Schulman GmbH
SCHULADUR® A GB 30 SCHWARZ PBT-GB30 A. Schulman GmbH
SCHULADUR® A GF 10 PBT-GF10 A. Schulman GmbH
SCHULADUR® A GF 15 HF FR 1 PBT-GF15 FR A. Schulman GmbH
SCHULADUR® A GF 15 HI PBT-I-GF15 A. Schulman GmbH
SCHULADUR® A GF 20 PBT-GF20 A. Schulman GmbH
SCHULADUR® A GF 20 HF FR 1 PBT-GF30 FR A. Schulman GmbH
SCHULADUR® A GF 30 PBT-GF30 A. Schulman GmbH
SCHULADUR® A GF 30 HF FR 1 PBT-GF30 FR A. Schulman GmbH
SCHULADUR® A GF 30 HF2 FR1 PBT-GF30 FR A. Schulman GmbH
SCHULADUR® A GF 30 HI PBT-I-GF30 A. Schulman GmbH
SCHULADUR® A GF 30 HIR SCHWARZ PBT-GF30 A. Schulman GmbH
SCHULADUR® A GF 30 TOP SPEED PBT-GF30 A. Schulman GmbH
SCHULADUR® A MV 14 PBT A. Schulman GmbH
SCHULADUR® A MV 14 FR 1 PBT FR A. Schulman GmbH
SCHULADUR® A MV 14 SHI FR 1 PBT-I FR A. Schulman GmbH
SCHULADUR® A NV 12 PBT A. Schulman GmbH
SCHULADUR® A NV 12 SHI PBT-I A. Schulman GmbH
SCHULADUR® A1 GF 30 HF FR 1 PBT-GF15 FR A. Schulman GmbH
SCHULADUR® A1 GF 30 LW (PBT+PET)-GF30... A. Schulman GmbH
SCHULADUR® A1 GF 50 (PBT+PET)-GF50 A. Schulman GmbH
SCHULADUR® A3 GF 10 (PBT+ASA)-GF10 A. Schulman GmbH
SCHULADUR® A3 GF 20 (ASA+PBT)-GF30... A. Schulman GmbH
SCHULADUR® A3 GF 30 (ASA+PBT)-GF30... A. Schulman GmbH
SCHULADUR® A3 GF 30 FR 1 (ASA+PBT)-GF30 FR... A. Schulman GmbH
SCHULADUR® A3 GF 30 TS SCHWARZ (PBT+ASA)-GF30 A. Schulman GmbH
SCHULADUR® PCR GF 15 K1947 (PBT+PET)-GF15 A. Schulman GmbH
SCHULADUR® PCR GF 20 (PBT+PET)-GF20... A. Schulman GmbH
SCHULADUR® PCR GF 30 (PBT+PET)-GF30... A. Schulman GmbH
SCHULADUR® PCR GF 45 (PBT+PET)-GF45... A. Schulman GmbH
SCHULATEC® TinCo 50 PBT-(MF(x)+Z)85 A. Schulman GmbH
Ultradur® B 2550 PBT BASF
Ultradur® B 2550 FC PBT BASF
Ultradur® B 4040 G10 (PBT+PET)-GF50 BASF
Ultradur® B 4040 G4 (PBT+PET)-GF20 BASF
Ultradur® B 4040 G6 (PBT+PET)-GF30 BASF
Ultradur® B 4040 G6 High Speed (PBT+PET)-GF30 BASF
Ultradur® B 4300 G10 PBT-GF50 BASF
Ultradur® B 4300 G2 PBT-GF10 BASF
Ultradur® B 4300 G2 FC PBT-GF10 BASF
Ultradur® B 4300 G2 High Speed PBT-GF10 BASF
Ultradur® B 4300 G3 High Speed PBT-GF15 BASF
Ultradur® B 4300 G4 PBT-GF20 BASF
Ultradur® B 4300 G4 FC PBT-GF20 BASF
Ultradur® B 4300 G4 High Speed PBT-GF20 BASF
Ultradur® B 4300 G6 PBT-GF30 BASF
Ultradur® B 4300 G6 FC Aqua UN PBT-GF30 BASF
Ultradur® B 4300 G6 High Speed PBT-GF30 BASF
Ultradur® B 4300 G6 HR PBT-GF30 BASF
Ultradur® B 4300 GM42 PBT-(GF+MF)30 BASF
Ultradur® B 4300 K4 PBT-GB20 BASF
Ultradur® B 4300 K6 PBT-GB30 BASF
Ultradur® B 4300 M5 PBT-MF25 BASF
Ultradur® B 4330 G6 HR PBT-I-GF30 BASF
Ultradur® B 4406 PBT FR BASF
Ultradur® B 4406 G2 PBT-GF10 FR BASF
Ultradur® B 4406 G4 PBT-GF20 FR BASF
Ultradur® B 4406 G6 PBT-GF30 FR BASF
Ultradur® B 4500 PBT BASF
Ultradur® B 4500 FC PBT BASF
Ultradur® B 4520 PBT BASF
Ultradur® B 4520 High Speed PBT BASF
Ultradur® B 4520 PRO PBT BASF
Ultradur® B 4560 PBT BASF
Ultradur® B 6550 PBT BASF
Ultradur® B 6550 FC PBT BASF
Ultradur® B 6550 L PBT BASF
Ultradur® B 6550 LN PBT BASF
Ultradur® S 4090 G2 (PBT+ASA)-GF10 BASF
Ultradur® S 4090 G4 (PBT+ASA)-GF20 BASF
Ultradur® S 4090 G4 High Speed (PBT+ASA)-GF20 BASF
Ultradur® S 4090 G6 (PBT+ASA)-GF30 BASF
Ultradur® S 4090 G6X (PBT+ASA)-GF30 BASF
Ultradur® S 4090 G6X High Speed (PBT+ASA)-GF30 BASF
Ultradur® S 4090 GX (PBT+ASA)-GF14 BASF
Ultradur® S 4090 GX LS High Speed (PBT+ASA)-GF14 BASF
VANDAR 2100 PBT Ticona
VANDAR 2100UV PBT Ticona
VANDAR 2122 PBT-P10 Ticona
VANDAR 2500 PBT Ticona
VANDAR 4602Z PBT Ticona
VANDAR 4602ZHR PBT Ticona
VANDAR 4612R PBT-GF7 Ticona
VANDAR 4632Z PBT-GF15 Ticona
VANDAR 4662Z PBT-GF30 Ticona
VANDAR 6000 PBT Ticona
VANDAR 8000 PBT Ticona
VESTODUR® 1000 nc (nf) PBT Evonik Industries AG
VESTODUR® 1003 nc (nf) PBT Evonik Industries AG
VESTODUR® 1003-FR3 nc (nf) PBT FR(17) Evonik Industries AG
VESTODUR® 2000 nc (nf) PBT Evonik Industries AG
VESTODUR® 2002-FR3 nc (nf) PBT FR(17) Evonik Industries AG
VESTODUR® 2003 nc (nf) PBT Evonik Industries AG
VESTODUR® 3000 nc (nf) PBT Evonik Industries AG
VESTODUR® 3001 nc (nf) PBT Evonik Industries AG
VESTODUR® 3013 nc (nf) PBT Evonik Industries AG
VESTODUR® 3030 nc (nf) PBT Evonik Industries AG
VESTODUR® GF10 nc (nf) PBT-GF10 Evonik Industries AG
VESTODUR® GF12-FR3 nc (nf) PBT-GF12 FR(17) Evonik Industries AG
VESTODUR® GF20 nc (nf) PBT-GF20 Evonik Industries AG
VESTODUR® GF20-FR3 nc (nf) PBT-GF20 FR(17) Evonik Industries AG
VESTODUR® GF30 nc (nf) PBT-GF30 Evonik Industries AG
VESTODUR® GF30-FR3 nc (nf) PBT-GF30 FR(17) Evonik Industries AG
VESTODUR® GK20 nc (nf) PBT-GB20 Evonik Industries AG
VESTODUR® GK30 nc (nf) PBT-GB20 Evonik Industries AG
VESTODUR® HI19 nc (nf) PBT-I Evonik Industries AG
VESTODUR® HI19-S3 nc (nf) PBT Evonik Industries AG
VESTODUR® X4621 PBT Evonik Industries AG
VESTODUR® X4877 nc (nf) PBT-I-GF30 Evonik Industries AG
VESTODUR® X7061 nc (nf) PBT Evonik Industries AG
VESTODUR® X7062 PBT Evonik Industries AG
VESTODUR® X7065 nc (nf) PBT Evonik Industries AG
VESTODUR® X7085 nc (nf) PBT-GF45 Evonik Industries AG
VESTODUR® X7095 nc (nf) PBT-GF Evonik Industries AG
VESTODUR® X7190 nc (nf) PBT Evonik Industries AG
VESTODUR® X7212 nc (nf) PBT-GF45 FR(17) Evonik Industries AG
VESTODUR® X7329 nc (nf) PBT-GF30 FR(17) Evonik Industries AG
VESTODUR® X7390 nc (nf) PBT Evonik Industries AG
VESTODUR® X7396 nc (nf) PBT Evonik Industries AG
VESTODUR® X9400 nc (nf) PBT-GF10 Evonik Industries AG
VESTODUR® X9402 blk (sw) E70127 PBT-GF30 Evonik Industries AG
VESTODUR® X9403 nc (nf) PBT FR(30) Evonik Industries AG
VESTODUR® X9405 nc (nf) PBT-GF30 FR(17) Evonik Industries AG
VESTODUR® X9417 blk (sw) E70286 PBT-GF15 Evonik Industries AG
VESTODUR® X9419 nc (nf) PBT Evonik Industries AG
VESTODUR® X9420 PBT Evonik Industries AG