CAMPUSplastics | All grades beginning with "M"

The international CAMPUS® database offers datasheets of the following materials with the selected first letter.

Please click on the grade of interest to generate a datasheet. You also may select a material by choosing a polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.


Grade Name Family Producer
Makroblend® DP7645 (PC+PET)-I Bayer MaterialScience
Makroblend® KU2-7609 (PC+PBT)-I-MD20 Bayer MaterialScience
Makroblend® KU2-7912/4 (PC+PBT)-I Bayer MaterialScience
Makroblend® KU2-7915 (PC+PBT)-I Bayer MaterialScience
Makroblend® S7916 (PBT+PC)-I Bayer MaterialScience
Makroblend® UT 403 (PC+PET)-I Bayer MaterialScience
Makroblend® UT1018 (PC+PBT) Bayer MaterialScience
Makroblend® UT203 (PC+PET)-I Bayer MaterialScience
Makroblend® UT235 M (PC+PET)-MD15 Bayer MaterialScience
Makroblend® UT250 (PC+PET)-I Bayer MaterialScience
Makroblend® UT305 (PC+PET) Bayer MaterialScience
Makroblend® UT3905 (PC+PBT)-I Bayer MaterialScience
Makroblend® UT3907 (PC+PBT)-I Bayer MaterialScience
Makroblend® UT4045 G (PC+PBT)-GF20 Bayer MaterialScience
Makroblend® UT408 (PC+PBT) Bayer MaterialScience
Makroblend® UT6005 (PC+PBT)-I Bayer MaterialScience
Makroblend® UT6007 (PC+PBT)-I Bayer MaterialScience
Makrolon® 1095 PC-GF15 Bayer MaterialScience
Makrolon® 1248 PC-I Bayer MaterialScience
Makrolon® 1260 PC-I Bayer MaterialScience
Makrolon® 1837 PC-I Bayer MaterialScience
Makrolon® 1837 GR PC Bayer MaterialScience
Makrolon® 1881 PC Bayer MaterialScience
Makrolon® 1885 PC Bayer MaterialScience
Makrolon® 1899 PC FR(40) Bayer MaterialScience
Makrolon® 1952 PC FR Bayer MaterialScience
Makrolon® 1954 PC Bayer MaterialScience
Makrolon® 2205 PC Bayer MaterialScience
Makrolon® 2207 PC Bayer MaterialScience
Makrolon® 2256 PC Bayer MaterialScience
Makrolon® 2258 PC Bayer MaterialScience
Makrolon® 2400 PC Bayer MaterialScience
Makrolon® 2405 PC Bayer MaterialScience
Makrolon® 2407 PC Bayer MaterialScience
Makrolon® 2456 PC Bayer MaterialScience
Makrolon® 2458 PC Bayer MaterialScience
Makrolon® 2467 PC FR Bayer MaterialScience
Makrolon® 2556 PC Bayer MaterialScience
Makrolon® 2558 PC Bayer MaterialScience
Makrolon® 2600 PC Bayer MaterialScience
Makrolon® 2605 PC Bayer MaterialScience
Makrolon® 2606 PC Bayer MaterialScience
Makrolon® 2607 PC Bayer MaterialScience
Makrolon® 2608 PC Bayer MaterialScience
Makrolon® 2652 PC Bayer MaterialScience
Makrolon® 2656 PC Bayer MaterialScience
Makrolon® 2658 PC Bayer MaterialScience
Makrolon® 2665 PC Bayer MaterialScience
Makrolon® 2667 PC FR Bayer MaterialScience
Makrolon® 2800 PC Bayer MaterialScience
Makrolon® 2805 PC Bayer MaterialScience
Makrolon® 2806 PC Bayer MaterialScience
Makrolon® 2807 PC Bayer MaterialScience
Makrolon® 2808 PC Bayer MaterialScience
Makrolon® 2856 PC Bayer MaterialScience
Makrolon® 2858 PC Bayer MaterialScience
Makrolon® 2865 PC FR Bayer MaterialScience
Makrolon® 2867 PC FR Bayer MaterialScience
Makrolon® 3100 PC Bayer MaterialScience
Makrolon® 3105 PC Bayer MaterialScience
Makrolon® 3106 PC Bayer MaterialScience
Makrolon® 3107 PC Bayer MaterialScience
Makrolon® 3152 PC Bayer MaterialScience
Makrolon® 3156 PC Bayer MaterialScience
Makrolon® 3206 PC Bayer MaterialScience
Makrolon® 3208 PC Bayer MaterialScience
Makrolon® 3258 PC Bayer MaterialScience
Makrolon® 6165 X PC FR Bayer MaterialScience
Makrolon® 6265 X PC FR Bayer MaterialScience
Makrolon® 6267 X PC FR Bayer MaterialScience
Makrolon® 6455 PC FR Bayer MaterialScience
Makrolon® 6457 PC FR Bayer MaterialScience
Makrolon® 6485 PC FR Bayer MaterialScience
Makrolon® 6487 PC FR Bayer MaterialScience
Makrolon® 6555 PC FR Bayer MaterialScience
Makrolon® 6557 PC FR Bayer MaterialScience
Makrolon® 6717 PC FR Bayer MaterialScience
Makrolon® 8025 PC-GF20 Bayer MaterialScience
Makrolon® 8035 PC-GF30 Bayer MaterialScience
Makrolon® 8325 PC-GF20 Bayer MaterialScience
Makrolon® 8345 PC-GF35 Bayer MaterialScience
Makrolon® 9125 PC-GF20 FR Bayer MaterialScience
Makrolon® 9415 PC-GF10 FR Bayer MaterialScience
Makrolon® 9417 PC-GF10 FR Bayer MaterialScience
Makrolon® 9425 PC-GF20 FR Bayer MaterialScience
Makrolon® AG2677 PC Bayer MaterialScience
Makrolon® AL2447 PC Bayer MaterialScience
Makrolon® AL2647 PC Bayer MaterialScience
Makrolon® DP1-1821 PC Bayer MaterialScience
Makrolon® ET IR320 PC Bayer MaterialScience
Makrolon® ET2613 PC Bayer MaterialScience
Makrolon® ET3113 PC Bayer MaterialScience
Makrolon® ET3117 PC Bayer MaterialScience
Makrolon® ET3127 PC Bayer MaterialScience
Makrolon® ET3227 PC Bayer MaterialScience
Makrolon® FR6901 PC FR Bayer MaterialScience
Makrolon® FR7067 PC FR Bayer MaterialScience
Makrolon® FR7087 PC FR Bayer MaterialScience
Makrolon® GF8001 PC-GF20 Bayer MaterialScience
Makrolon® GF8002 PC-GF15 Bayer MaterialScience
Makrolon® GF9002 PC-GF10 Bayer MaterialScience
Makrolon® LED2045 PC Bayer MaterialScience
Makrolon® LED2245 PC Bayer MaterialScience
Makrolon® LED2643 PC Bayer MaterialScience
Makrolon® LQ2647 PC Bayer MaterialScience
Makrolon® LQ3187 PC Bayer MaterialScience
Makrolon® LTG2623 PC Bayer MaterialScience
Makrolon® OD2015 PC Bayer MaterialScience
Makrolon® Rx1452 PC Bayer MaterialScience
Makrolon® Rx1805 PC Bayer MaterialScience
Makrolon® Rx1851 PC Bayer MaterialScience
Makrolon® Rx2430 PC Bayer MaterialScience
Makrolon® Rx2435 PC Bayer MaterialScience
Makrolon® Rx2530 PC Bayer MaterialScience
Makrolon® Rx2635 PC Bayer MaterialScience
Makrolon® SF800 Z MAS148 PC-GF5 Bayer MaterialScience
Makrolon® SF805 PC-GF5 Bayer MaterialScience
Makrolon® SF810 PC-GF10 Bayer MaterialScience
Makrolon® WB1239 PC Bayer MaterialScience
Makrolon® XT5010 PC Bayer MaterialScience
Minlon® 10B140 BK061 PA66-MD40 DuPont Engineering Polymers
Minlon® 10B40 NC010 PA66-MD40 DuPont Engineering Polymers
Minlon® 10B40HS1 BK061 PA66-MD40 DuPont Engineering Polymers
Minlon® 11C140 NC010 PA66-I-MD40 DuPont Engineering Polymers
Minlon® 11C40 NC010 PA66-I-MD40 DuPont Engineering Polymers
Minlon® 12T NC010 PA66-I-MD36 DuPont Engineering Polymers
Minlon® 12TA BKB124 PA66-I-MD32 DuPont Engineering Polymers
Minlon® 22C NC010 PA66-(MD+GF)38 DuPont Engineering Polymers
Minlon® 73GM40 NC010 PA6-(MD+GF)40 DuPont Engineering Polymers
Minlon® 73M30 NC010 PA6-MD30 DuPont Engineering Polymers
Minlon® 73M40 NC010 PA6-MD40 DuPont Engineering Polymers
Minlon® EFE6053 BK413 PA66-(MD+GF)40 DuPont Engineering Polymers
Minlon® EFE6096 GY090A PA66-I-MD15 DuPont Engineering Polymers
Minlon® FE6190 BK086 PA66-(MD+GF)36 DuPont Engineering Polymers
Minlon® IG38C1 BK434 PA66-(MD+GF)38 DuPont Engineering Polymers