| Propriedades reológicas | Valor | Unidade | Método de ensaio |
| Índice de fluidez volumétrico, MVR | 17 | cm³/10min | ISO 1133 |
| Temperatura | 300 | °C | ISO 1133 |
| Carga | 1.2 | kg | ISO 1133 |
| Propriedades mecânicas | Valor | Unidade | Método de ensaio |
| Módulo de tração | 2400 | MPa | ISO 527-1/-2 |
| Tensão no escoamento | 66 | MPa | ISO 527-1/-2 |
| Deformação no escoamento | 6 | % | ISO 527-1/-2 |
| Resistência ao impacto Charpy , +23°C | N | kJ/m² | ISO 179/1eU |
| Res. impacto Charpy c/entalhe, +23°C | 11 | kJ/m² | ISO 179/1eA |
| Propriedades térmicas | Valor | Unidade | Método de ensaio |
| Temperatura de deflexão térmica, 1.80 MPa | 124 | °C | ISO 75-1/-2 |
| Temperatura de amolecimento Vicat, 50°C/h 50N | 142 | °C | ISO 306 |
| Flamabilidade a 1.5mm esp. nom. | HB | class | IEC 60695-11-10 |
| Espessuras do tubo de teste | 1.5 | mm | IEC 60695-11-10 |
| Flamabilidade a espessura h | V-2 | class | IEC 60695-11-10 |
| Espessuras do tubo de teste | 0.8 | mm | IEC 60695-11-10 |
| Outras propriedades | Valor | Unidade | Método de ensaio |
| Densidade | 1200 | kg/m³ | ISO 1183 |
Características
Processamento
Moldagem por injeção
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Any information given on the chemical and physical characteristics of our products, including technical advice on applications whether verbally, in writing or by testing the product, is given to the best of our knowledge, but without warranty. It does not exempt the buyer from carrying out his own investigations and tests in order to ascertain the products' specific suitability for the purpose intended. The buyer is solely responsible for the application, utilisation and processing of the products, and must observe the laws and government regulations and the consequential rights of any third party. At all times our Conditions of Sale apply. The test values given are guide values, not binding minimum or maximum figures, which have been determined on standardized test specimen and can be affected by pigmentation, mold design and processing conditions.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012