CAMPUS® datasheet | ALTECH PA66 A 4040/100 MR40


This datasheet of ALTECH PA66 A 4040/100 MR40 from ALBIS Plastic GmbH is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

  ALTECH PA66 A 4040/100 MR40 | PA66-MX40 | ALBIS Plastic GmbH
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
Módulo de tração 6500 / 4500 MPa ISO 527-1/-2
Tensão na ruptura 90 / 75 MPa ISO 527-1/-2
Deformação na ruptura 6 / 15 % ISO 527-1/-2
Resistência ao impacto Charpy , +23°C 80 / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 4 / - kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
Temperatura de fusão, 10°C/min 253 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 120 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 235 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, 50°C/h 50N 200 / * °C ISO 306
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
Resistividade volumétrica específica 1E13 / 1E10 Ohm*m IEC 60093
Resistividade superficial específica * / 1E12 Ohm IEC 60093
Índice comparativo de linha de fuga 550 / - - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 5 / * % Sim. to ISO 62
Absorção de umidade 1.3 / * % Sim. to ISO 62
Densidade 1500 / - kg/m³ ISO 1183
Características
Processamento
Moldagem por injeção
Características especiais
Estável contra o calor
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012