CAMPUS® datasheet | Kynar® FLEX 3120-50
This datasheet of Kynar® FLEX 3120-50 from ARKEMA is provided by the international plastics database CAMPUS.
Kynar® FLEX 3120-50 | PVDF | ARKEMA
Informação do produto
Kynar® FLEX 3120-50
Kynar® FLEX are fluorinated thermoplastic copolymers.
Outstanding characteristics of Kynar® FLEX : chemical resistance,
imperviousness to UV, high barrier properties, high purity,good mechanical
and thermomechanical properties.
Main applications of Kynar® FLEX : corrosion protection in the chemical
industry, coating (painting, extrusion), wire and cable.
Kynar® FLEX 3120-50 is a grade which exhibits, compared to 2800,
a higher melting point which allows a greater range for use.
For cable coating, extrusion of tube and plaque, compression moulding
of bulky parts.
| Propriedades reológicas | Valor | Unidade | Método de ensaio |
| Índice de fluidez volumétrico, MVR | 0.5 | cm³/10min | ISO 1133 |
| Temperatura | 230 | °C | ISO 1133 |
| Carga | 5 | kg | ISO 1133 |
| Propriedades mecânicas | Valor | Unidade | Método de ensaio |
| Módulo de tração | 690 | MPa | ISO 527-1/-2 |
| Tensão no escoamento | 28 | MPa | ISO 527-1/-2 |
| Deformação no escoamento | 12 | % | ISO 527-1/-2 |
| Deformação nominal na ruptura | >50 | % | ISO 527-1/-2 |
| Propriedades térmicas | Valor | Unidade | Método de ensaio |
| Temperatura de fusão, 10°C/min | 165 | °C | ISO 11357-1/-3 |
| Temp. de transição vítrea, 10°C/min | -46 | °C | ISO 11357-1/-2 |
| Outras propriedades | Valor | Unidade | Método de ensaio |
| Densidade | 1780 | kg/m³ | ISO 1183 |
| Produção de amostra para teste | Valor | Unidade | Método de ensaio |
| Moldagem por compressão, temperatura do molde | 225 | °C | ISO 293 |
| Moldagem por compressão, tempo de moldagem | 3 | min | ISO 293 |
| Moldagem por compressão, temperatura de desmoldagem | 120 | °C | ISO 293 |
Características
Processamento
Extrusão de perfis, Outros tipos de extrusão
Forma de entrega
Granulos
Características especiais
Estável a luz, Estabilidade a raios U.V./Intempéries, Estável contra o calor
Disponibilidade regional
Resistência em meio químico
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.
The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.
For information about the other products marketed
by our company consult :
ARKEMA,
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012