CAMPUS® datasheet | Minlon® 10B40HS1 BK061
This datasheet of Minlon® 10B40HS1 BK061 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.
Grades with improved electrical and flammability properties are available within the Zytel® nylon resin product line. In addition, Minlon® nylon resin is available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses.
The good melt stability of Minlon® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.
Minlon® nylon resin typically is used in demanding applications in the automotive, electrical, electronic, domestic appliances and construction industries.
Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.
| Propriedades reológicas | Seco / Cond | Unidade | Método de ensaio |
| Contração após a moldagem, paralelo | 0.4 / * | % | ISO 294-4, 2577 |
| Contração após a moldagem, perpendicular | 0.9 / * | % | ISO 294-4, 2577 |
| Propriedades mecânicas | Seco / Cond | Unidade | Método de ensaio |
| Módulo de tração | 10000 / - | MPa | ISO 527-1/-2 |
| Tensão na ruptura | 95 / - | MPa | ISO 527-1/-2 |
| Deformação na ruptura | 2.5 / - | % | ISO 527-1/-2 |
| Res. impacto Charpy c/entalhe, +23°C | 3 / - | kJ/m² | ISO 179/1eA |
| Propriedades térmicas | Seco / Cond | Unidade | Método de ensaio |
| Temperatura de fusão, 10°C/min | 263 / * | °C | ISO 11357-1/-3 |
| Temperatura de deflexão térmica, 1.80 MPa | 170 / * | °C | ISO 75-1/-2 |
| Temperatura de deflexão térmica, 0.45 MPa | 240 / * | °C | ISO 75-1/-2 |
| Coef. de expansão térmica linear, paralelo | 36 / * | E-6/K | ISO 11359-1/-2 |
| Coef. de expansão térmica linear, perpend. | 66 / * | E-6/K | ISO 11359-1/-2 |
| Outras propriedades | Seco / Cond | Unidade | Método de ensaio |
| Densidade | 1510 / - | kg/m³ | ISO 1183 |
Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.
The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.
The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.
CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.
For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012