POLYMAN® (ABS) LP 137 A | ABS | A. Schulman GmbH
Informação do produto
Impact ABS grade with antistatic
| Propriedades reológicas | Valor | Unidade | Método de ensaio |
| Índice de fluidez volumétrico, MVR | 22 | cm³/10min | ISO 1133 |
| Temperatura | 220 | °C | ISO 1133 |
| Carga | 10 | kg | ISO 1133 |
| Propriedades mecânicas | Valor | Unidade | Método de ensaio |
| Módulo de tração | 2200 | MPa | ISO 527-1/-2 |
| Tensão no escoamento | 48 | MPa | ISO 527-1/-2 |
| Deformação no escoamento | 2.3 | % | ISO 527-1/-2 |
| Resistência ao impacto Charpy , +23°C | N | kJ/m² | ISO 179/1eU |
| Res. impacto Charpy c/entalhe, +23°C | 18 | kJ/m² | ISO 179/1eA |
| Propriedades térmicas | Valor | Unidade | Método de ensaio |
| Temperatura de amolecimento Vicat, 50°C/h 50N | 96 | °C | ISO 306 |
| Flamabilidade a 1.5mm esp. nom. | HB | class | IEC 60695-11-10 |
| Espessuras do tubo de teste | 1.5 | mm | IEC 60695-11-10 |
| Recognição UL | UL | - | - |
| Propriedades elétricas | Valor | Unidade | Método de ensaio |
| Resistividade volumétrica específica | >1E13 | Ohm*m | IEC 60093 |
| Resistividade superficial específica | >1E15 | Ohm | IEC 60093 |
| Outras propriedades | Valor | Unidade | Método de ensaio |
| Densidade | 1050 | kg/m³ | ISO 1183 |
Diagrama
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulado
Características especiais
Antiestático
Disponibilidade regional
Disclaimer
The information and recommendations contained in this document are based upon
data collected by A. Schulman and are believed to be reliable; however, because
A. Schulman cannot anticipate or control the many different conditions under
which this information and/or product may be used, no representation is made
and no warranty is given of any kind, express or implied, for completeness,
accuracy, availability, suitability, usefulness, commercial value, or non-violation
of intellectual property rights of information, recommendations, and products
and services directly or indirectly provided. A. Schulman assumes no responsibility
for the results of the use of products and processes described herein and expressly
disclaims the implied warranties of merchantability and fitness for a particular use
If there are questions to given information, to further properties or further A. Schulman
products please contact
A. Schulman GmbH
Huettenstrasse 211
50170 Kerpen
Tel: 02273 / 561-0
Contact: aschulman@de.aschulman.com
Subject: Material data
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012