Informação do produto
Injection-moulding grade with 30% glass-fibres; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors and housings for electronic units under the hood.
Abbreviated designation according to ISO 1043-1: PBT
CLASSIFICATION ACCORDING TO ISO 7792-1:
Moulding Compound ISO 7792-PBT, MGHLPRW, 11-090, GF30
Abbreviated designation according to ISO 1043-1: PBT
CLASSIFICATION ACCORDING TO ISO 7792-1:
Moulding Compound ISO 7792-PBT, MGHLPRW, 11-090, GF30
| Propriedades reológicas | Valor | Unidade | Método de ensaio |
| Índice de fluidez volumétrico, MVR | 5.5 | cm³/10min | ISO 1133 |
| Temperatura | 250 | °C | ISO 1133 |
| Carga | 2.16 | kg | ISO 1133 |
| Contração após a moldagem, paralelo | 0.5 | % | ISO 294-4, 2577 |
| Contração após a moldagem, perpendicular | 1.3 | % | ISO 294-4, 2577 |
| Propriedades mecânicas | Valor | Unidade | Método de ensaio |
| Módulo de tração | 8700 | MPa | ISO 527-1/-2 |
| Tensão na ruptura | 130 | MPa | ISO 527-1/-2 |
| Deformação na ruptura | 3.3 | % | ISO 527-1/-2 |
| Resistência ao impacto Charpy , +23°C | 70 | kJ/m² | ISO 179/1eU |
| Res. impacto Charpy c/entalhe, +23°C | 12 | kJ/m² | ISO 179/1eA |
| Propriedades térmicas | Valor | Unidade | Método de ensaio |
| Temperatura de fusão, 10°C/min | 223 | °C | ISO 11357-1/-3 |
| Temperatura de deflexão térmica, 1.80 MPa | 205 | °C | ISO 75-1/-2 |
| Temperatura de deflexão térmica, 0.45 MPa | 220 | °C | ISO 75-1/-2 |
| Propriedades elétricas | Valor | Unidade | Método de ensaio |
| Resistência elétrica | 37 | kV/mm | IEC 60243-1 |
| Outras propriedades | Valor | Unidade | Método de ensaio |
| Absorção de água | 0.4 | % | Sim. to ISO 62 |
| Absorção de umidade | 0.2 | % | Sim. to ISO 62 |
| Densidade | 1510 | kg/m³ | ISO 1183 |
| Propriedades específicas do material | Valor | Unidade | Método de ensaio |
| Índice de viscosidade | 108 | cm³/g | ISO 307, 1157, 1628 |
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Disponibilidade regional
Resistência em meio químico
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact your local BASF
representative or
BASF SE
Dept. PM/K
Fax: 0621-60-49497
e-mail: e-mail
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact your local BASF
representative or
BASF SE
Dept. PM/K
Fax: 0621-60-49497
e-mail: e-mail
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012