Informação do produto
Very free-flowing, rapidly solidifying grade for use where processing is extremely difficult but mechanical properties are lower.
Abbreviated designation according to ISO 1043: POM
Designation according to ISO 9988-1: POM-K, M-GNR, 05-002
Abbreviated designation according to ISO 1043: POM
Designation according to ISO 9988-1: POM-K, M-GNR, 05-002
| Propriedades reológicas | Valor | Unidade | Método de ensaio |
| Índice de fluidez volumétrico, MVR | 25 | cm³/10min | ISO 1133 |
| Temperatura | 190 | °C | ISO 1133 |
| Carga | 2.16 | kg | ISO 1133 |
| Propriedades mecânicas | Valor | Unidade | Método de ensaio |
| Módulo de tração | 2800 | MPa | ISO 527-1/-2 |
| Tensão no escoamento | 65 | MPa | ISO 527-1/-2 |
| Deformação no escoamento | 7.5 | % | ISO 527-1/-2 |
| Deformação nominal na ruptura | 24 | % | ISO 527-1/-2 |
| Módulo de tensão de fluência, 1h | 2100 | MPa | ISO 899-1 |
| Módulo de tensão de fluência, 1000h | 1350 | MPa | ISO 899-1 |
| Resistência ao impacto Charpy , +23°C | 150 | kJ/m² | ISO 179/1eU |
| Resistência ao impacto Charpy, -30°C | 150 | kJ/m² | ISO 179/1eU |
| Res. impacto Charpy c/entalhe, +23°C | 5 | kJ/m² | ISO 179/1eA |
| Res. impacto Charpy c/entalhe, -30°C | 4 | kJ/m² | ISO 179/1eA |
| Propriedades térmicas | Valor | Unidade | Método de ensaio |
| Temperatura de fusão, 10°C/min | 167 | °C | ISO 11357-1/-3 |
| Temperatura de deflexão térmica, 1.80 MPa | 100 | °C | ISO 75-1/-2 |
| Temperatura de deflexão térmica, 0.45 MPa | 156 | °C | ISO 75-1/-2 |
| Temperatura de amolecimento Vicat, 50°C/h 50N | 150 | °C | ISO 306 |
| Coef. de expansão térmica linear, paralelo | 110 | E-6/K | ISO 11359-1/-2 |
| Flamabilidade a 1.5mm esp. nom. | HB | class | IEC 60695-11-10 |
| Espessuras do tubo de teste | 1.6 | mm | IEC 60695-11-10 |
| Recognição UL | UL | - | - |
| Flamabilidade a espessura h | HB | class | IEC 60695-11-10 |
| Espessuras do tubo de teste | 0.8 | mm | IEC 60695-11-10 |
| Recognição UL | UL | - | - |
| Flamabilidade conforme índice de oxigênio | 15 | % | ISO 4589-1/-2 |
| Propriedades elétricas | Valor | Unidade | Método de ensaio |
| Constante dielétrica, 100Hz | 3.8 | - | IEC 60250 |
| Constante dielétrica, 1MHz | 3.8 | - | IEC 60250 |
| Fator de dissipação dielétrica, 100Hz | 10 | E-4 | IEC 60250 |
| Fator de dissipação dielétrica, 1MHz | 50 | E-4 | IEC 60250 |
| Resistividade volumétrica específica | 1E13 | Ohm*m | IEC 60093 |
| Resistividade superficial específica | 1E13 | Ohm | IEC 60093 |
| Resistência elétrica | 40 | kV/mm | IEC 60243-1 |
| Índice comparativo de linha de fuga | 600 | - | IEC 60112 |
| Outras propriedades | Valor | Unidade | Método de ensaio |
| Absorção de água | 0.8 | % | Sim. to ISO 62 |
| Absorção de umidade | 0.2 | % | Sim. to ISO 62 |
| Densidade | 1400 | kg/m³ | ISO 1183 |
| Propriedades para cálculos reológicos | Valor | Unidade | Método de ensaio |
| Temperatura de ejeção | 110 | °C | - |
| Produção de amostra para teste | Valor | Unidade | Método de ensaio |
| Moldagem por injeção, temperatura da massa | 200 | °C | ISO 294 |
| Moldagem por injeção, temperatura do molde | 90 | °C | ISO 10724 |
| Moldagem por injeção, velocidade de injeção | 200 | mm/s | ISO 294 |
Diagrama
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Aditivos
Desmoldante
Disponibilidade regional
Resistência em meio químico
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact your local BASF
representative or
BASF SE
Dept. PM/K
Fax: 0621-60-49497
e-mail: e-mail
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact your local BASF
representative or
BASF SE
Dept. PM/K
Fax: 0621-60-49497
e-mail: e-mail
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012