  VESTAMID® L-R1-MHI blk (sw) | PA12 | Evonik Industries AG
Informação do produto
VESTAMID® L-R1-MHI blk

 

Resin: ISO 1874-PA12-HI, MHZ, 16-020  

 

VESTAMID® L-R1-MHI is particularly characterized by the following material properties:

  • electrically conductive
  • medium-viscosity
  • heat and light stabilized
  • increased low-temperatur impact strength
  • with processing aid


The resistance values of the finished parts are dependent on the processing conditions.


Application examples: Antistatic and electrically conductive moldings or extrudates for

                                    use in areas prone to explosions.

Propriedades reológicasValorUnidadeMétodo de ensaio
Contração após a moldagem, paralelo 1.7 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.7 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
Módulo de tração 1600 MPa ISO 527-1/-2
Tensão no escoamento 37 MPa ISO 527-1/-2
Deformação no escoamento 5 % ISO 527-1/-2
Deformação nominal na ruptura 45 % ISO 527-1/-2
Resistência ao impacto Charpy , +23°C N kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 80 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 60 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 8 kJ/m² ISO 179/1eA
Propriedades térmicasValorUnidadeMétodo de ensaio
Temperatura de fusão, 10°C/min 178 °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 50 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 130 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, 50°C/h 50N 140 °C ISO 306
Flamabilidade a 1.5mm esp. nom. HB class IEC 60695-11-10
Espessuras do tubo de teste 1.6 mm IEC 60695-11-10
Flamabilidade a espessura h HB class IEC 60695-11-10
Espessuras do tubo de teste 3.2 mm IEC 60695-11-10
Propriedades elétricasValorUnidadeMétodo de ensaio
Resistividade volumétrica específica 0.1 Ohm*m IEC 60093
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água 1.4 % Sim. to ISO 62
Absorção de umidade 0.5 % Sim. to ISO 62
Densidade 1110 kg/m³ ISO 1183
Produção de amostra para testeValorUnidadeMétodo de ensaio
Moldagem por injeção, temperatura da massa 270 °C ISO 294
Moldagem por injeção, temperatura do molde 80 °C ISO 10724
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Moldagem por injeção, pressão de recalque 70 MPa ISO 294
Características
Processamento
Moldagem por injeção
Disponibilidade regional
Disclaimer
All listed technical data are typical values intended for your guidance.
They are given without obligation and do not constitute a materials
specification. Should you have any further questions concerning material
behavior or properties, please contact us at the following address :

for PA:           Evonik Industries AG
                     PP-HP-CRM
                     Gebäude 1227 / PB 16
                     D-45764 Marl
                     Phone: +49-(0)2365/49-2720
                     Fax:+49-(0)2365/49-2070
                     E-Mail: campusplastics@evonik.com

for PMMA:     Evonik Industries AG
                     Marketing / Campus
                     Kirschenallee
                     D-64293 Darmstadt
                     Germany
                     Phone: +49 - (0) 61 51 / 18-47 11
                     Fax: +49 - (0) 61 51 / 18-31 77
                     E-Mail: campusplastics@evonik.com
                     Internet: http://www.plexiglas-polymers.com

 

® = registered trademark

 

PLEXIGLAS® is a registered trademark of Evonik Röhm GmbH, Germany,

outside of the Americas. Within the Americas it is sold as ACRYLITE®,

which is a registered trademark of Evonik Cyro LLC, USA.

PLEXIMID® is a registered trademarks of Evonik Röhm GmbH, Germany.

CYROLITE® and XT® polymer are registered trademarks of Evonik Cyro LLC, USA.

 

This information and all further technical advice is based on our present knowledge

and experience. However, it implies no liability or other legal responsibility on our part,

including with regard to existing third party intellectual property rights, especially

patent rights. In particular, no warranty, whether express or implied, or guarantee of

product properties in the legal sense is intended or implied. We reserve the right to

make any changes according to technological progress or further developments. The

customer is not released from the obligation to conduct careful inspection and testing

of incoming goods. Performance of the product described herein should be verified by

testing, which should be carried out only by qualified experts in the sole responsibility

of a customer. Reference to trade names used by other companies is neither a

recommendation, nor does it imply that similar products could not be used.

 

NAFTA:

This information and all technical and other advice are based on Evonik’s

present knowledge and experience. However, Evonik assumes no liability for

such information or advice, including the extent to which such information or

advice may relate to third party intellectual property rights. Evonik reserves the

right to make any changes to information or advice at any time, without prior

or subsequent notice. EVONIK DISCLAIMS ALL REPRESENTATIONS AND

WARRANTIES, WHETHER EXPRESS OR IMPLIED, AND SHALL HAVE NO LIABILITY

FOR, MERCHANTABILITY OF THE PRODUCT OR ITS FITNESS FOR A PARTICULAR

PURPOSE (EVEN IF EVONIK IS AWARE OF SUCH PURPOSE), OR OTHERWISE.

EVONIK SHALL NOT BE RESPONSIBLE FOR CONSEQUENTIAL, INDIRECT OR

INCIDENTAL DAMAGES (INCLUDING LOSS OF PROFITS) OF ANY KIND. It is the

customer’s sole responsibility to arrange for inspection and testing of all

products by qualified experts. Reference to trade names used by other

companies is neither a recommendation nor an endorsement of the

corresponding product, and does not imply that similar products could not be

used.

 

Sales range and technical data subject to alteration.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012