| Механические свойства | Значение | Единица | Стандарт |
| Напряжение при 100%-ном растяжении | 2.2 | МПа | ISO 527-1/-2 |
| Удлинение при разрыве ТЭП | >300 | % | ISO 527-1/-2 |
| Остаточная деформация при постоянной нагрузке, 100°C | 37 | % | ISO 815 |
| Стойкость к разрыву | 23 | кН/м | ISO 34-1 |
| Твердость по Шору А, 3 сек | 60 | - | ISO 868 |
| Прочие свойства | Значение | Единица | Стандарт |
| Плотность | 960 | кг/м³ | ISO 1183 |
Особые свойства и характеристики
Способы переработки
Литье под давлением, Экструзия (прочие виды)
Особые показатели
Стабилизированный к УФ или погодостойкий
Доступность материала по регионам
Северная Америка, Европа, Страны Азии и Тихого океана, Латинская Америка, Ближний Восток и Африка
Дискламация
Any information given on the chemical and physical characteristics of our products, including technical advice on applications whether verbally, in writing or by testing the product, is given to the best of our knowledge, but without warranty. It does not exempt the buyer from carrying out his own investigations and tests in order to ascertain the products' specific suitability for the purpose intended. The buyer is solely responsible for the application, utilisation and processing of the products, and must observe the laws and government regulations and the consequential rights of any third party. At all times our Conditions of Sale apply. The test values given are guide values, not binding minimum or maximum figures, which have been determined on standardized test specimen and can be affected by pigmentation, mold design and processing conditions.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012