general-purpose injection molding grade
20% minerals
| Механические свойства | сухой / конд | Единица | Стандарт |
| Модуль упругости при растяжении | 4000 / 1700 | МПа | ISO 527-1/-2 |
| Напряжение при разрыве | 75 / 40 | МПа | ISO 527-1/-2 |
| Удлинение при разрыве | 19 / 50 | % | ISO 527-1/-2 |
| Ударная вязкость по Шарпи, +23°C | N / N | кДж/м2 | ISO 179/1eU |
| Ударная вязкость по Шарпи с надрезом, +23°C | 9 / 20 | кДж/м2 | ISO 179/1eA |
| Ударная вязкость по Шарпи с надрезом, -30°C | 7 / - | кДж/м2 | ISO 179/1eA |
| Теплофизические свойства | сухой / конд | Единица | Стандарт |
| Температура плавления, 10°C/мин | 223 / * | °C | ISO 11357-1/-3 |
| Температура изгиба под нагрузкой, 1.80 МПа | 60 / * | °C | ISO 75-1/-2 |
| Температура изгиба под нагрузкой, 0.45 МПа | 190 / * | °C | ISO 75-1/-2 |
| Класс горючести при номинальной толщине 1.5 мм | HB / * | класс | IEC 60695-11-10 |
| Толщина образца | 1.6 / * | мм | IEC 60695-11-10 |
| Класс горючести при толщине образца h | HB / * | класс | IEC 60695-11-10 |
| Толщина образца | 0.8 / * | мм | IEC 60695-11-10 |
| Электрические свойства | сухой / конд | Единица | Стандарт |
| Относительная диэлектрическая проницаемость, 1МГц | 3.8 / 6.2 | - | IEC 60250 |
| Коэффициент диэлектрических потерь, 1 MГц | 200 / 2000 | E-4 | IEC 60250 |
| Удельное объемное сопротивление | 1E13 / 1E10 | Ом*м | IEC 60093 |
| Удельное поверхностное сопротивление | * / 1E10 | Ом | IEC 60093 |
| Сравнительный показатель пробоя | - / 500 | - | IEC 60112 |
| Прочие свойства | сухой / конд | Единица | Стандарт |
| Водопоглощение | 5.7 / * | % | Sim. to ISO 62 |
| Поглощение влаги | 1.8 / * | % | Sim. to ISO 62 |
| Плотность | 1280 / - | кг/м³ | ISO 1183 |
| Особые свойства материала | сухой / конд | Единица | Стандарт |
| Коэффициент вязкости | 150 / * | см³/г | ISO 307, 1157, 1628 |
| Параметры изготовления образцов для испытаний | Значение | Единица | Стандарт |
| Литье под давлением, температура расплава | 270 | °C | ISO 294 |
| Литье под давлением, температура пресс-формы | 80 | °C | ISO 10724 |
PolyOnePolyOne Engineered Materials Europe
PolyOne Th.Bergmann GmbH
PolyOne Corporation makes no representations, guarantees or warranties of any kind with respect to the information contained in this document about its accuracy, suitability for particular applications ort he result obtained or obtainable using the information. Some of the information arises from laboratory work with small-case equipment which may not provide a reliable indication of performance or properties obtained or obtainable on larger-scale equipment. Processing conditions can cause material properties to shift from the values stated in data bases. PolyOne Corporation makes no guarantees or warranties respecting suitability of either PolyOne’s products or the information for your process or end-use application. You have the responsibility to conduct full-scale end-product performance testing to determine suitability in your application, and you assume all risks and liability arising from your use of the information and/or handling of any product. PolyOne Corporation makes no warranties, express or implied, including, but not limited to, implied warranties of merchantability and fitness for a particular purpose, either with respect to the information or products reflected by the information. These information shall not operate as permission, recommendation or inducement to practice any patented invention without permission of the patent owner.
Germany:
PolyOne Th.Bergmann GmbH
Adolf-Dambach-Strasse 2-4
D-76571 Gaggenau
Tel.: 07225 6802 0
Fax:07225 6802 10
France:
PolyOne Engineered Materials SA, FRANCE
20, Rue Salvador Allende, BP 105
42353 La Talaudière Cedex, France
Tel.: +33 (0) 477 47 64 00
Tel.:+33 (0) 477 57 13
Spain:
Pol. Ind. Valle del Cinca
22300 Barbastro, Spain
Tel.: +34 (0) 974 31 03 14
Fax.: +34 (0) 974 31 43 11
United Kingdom:
PolyOne Engineered Materials UL Ltd.
Newton Ayecliff
Durham DL5 6EA, UK
Tel.:+44 (0) 1325 30 08 48
Fax.:+44 (0) 1325 30 14 13
Turkey:
Tekno Polimer
103 Kücükcekmece
Istanbul, Turkey
Tel:+90 212 549 2256
Fax.:+90 212 549 2241
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012