CAMPUS® datasheet | Delrin® FG400XRD NC010
This datasheet of Delrin® FG400XRD NC010 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.
The good melt stability of Delrin® acetal resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-17 kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.
Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics and consumer goods industries.
Delrin® FG400XRD NC010 is a filled, medium viscosity acetal copolymer for injection molding. It is detected in x-ray detectors. It has been developed for consideration into applications such as parts for the food industry.
| Реологические свойства | Значение | Единица | Стандарт |
| Показатель текучести расплава, ПТР | 8 | см³/10мин | ISO 1133 |
| Температура | 190 | °C | ISO 1133 |
| Нагрузка | 2.16 | кг | ISO 1133 |
| Механические свойства | Значение | Единица | Стандарт |
| Модуль упругости при растяжении | 3200 | МПа | ISO 527-1/-2 |
| Напряжение в точке текучести | 51 | МПа | ISO 527-1/-2 |
| Удлинение в точке текучести | 7 | % | ISO 527-1/-2 |
| Номинальное удлинение при разрыве | 15 | % | ISO 527-1/-2 |
| Ударная вязкость по Шарпи, +23°C | 80 | кДж/м2 | ISO 179/1eU |
| Ударная вязкость по Шарпи с надрезом, +23°C | 4 | кДж/м2 | ISO 179/1eA |
| Теплофизические свойства | Значение | Единица | Стандарт |
| Температура плавления, 10°C/мин | 168 | °C | ISO 11357-1/-3 |
| Коэффициент линейного теплового расширения, продольный | 120 | E-6/K | ISO 11359-1/-2 |
| Коэффициент линейного теплового расширения, поперечный | 120 | E-6/K | ISO 11359-1/-2 |
| Класс горючести при номинальной толщине 1.5 мм | HB | класс | IEC 60695-11-10 |
| Толщина образца | 1.5 | мм | IEC 60695-11-10 |
| Параметры для расчета реологических свойств | Значение | Единица | Стандарт |
| Плотность расплава | 1420 | кг/м³ | - |
Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.
The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2013 E.I. du Pont de Nemours and Company. All Rights Reserved.
The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.
CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.
For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012