View list of
CAMPUS® datasheet | Durethan® BC 700 HTS
This datasheet of Durethan® BC 700 HTS from LANXESS Deutschland GmbH is provided by the international plastics database CAMPUS.
Durethan® BC 700 HTS | PA6-I | LANXESS Deutschland GmbH
Описание продукта
PA 6, non-reinforced, extrusion, Blasform, impact modified, heat-ageing stabilized
| Механические свойства | сухой / конд | Единица | Стандарт |
| Модуль упругости при растяжении | 980 / 210 | МПа | ISO 527-1/-2 |
| Напряжение в точке текучести | 28 / - | МПа | ISO 527-1/-2 |
| Удлинение в точке текучести | 6.5 / - | % | ISO 527-1/-2 |
| Ударная вязкость по Шарпи, -30°C | 105 / - | кДж/м2 | ISO 179/1eU |
| Теплофизические свойства | сухой / конд | Единица | Стандарт |
| Температура плавления, 10°C/мин | 211 / * | °C | ISO 11357-1/-3 |
| Температура изгиба под нагрузкой, 1.80 МПа | 48 / * | °C | ISO 75-1/-2 |
| Температура изгиба под нагрузкой, 0.45 МПа | 53 / * | °C | ISO 75-1/-2 |
| Коэффициент линейного теплового расширения, продольный | 200 / * | E-6/K | ISO 11359-1/-2 |
| Коэффициент линейного теплового расширения, поперечный | 200 / * | E-6/K | ISO 11359-1/-2 |
| Прочие свойства | сухой / конд | Единица | Стандарт |
| Плотность | 1030 / - | кг/м³ | ISO 1183 |
Особые свойства и характеристики
Способы переработки
Выдувное формование
Вид поставки
Гранулы
Добавки
Смазочные добавки
Особые показатели
Термостабилизированный или стойкий к воздействию тепла
Доступность материала по регионам
Дискламация
This information and our technical advice - whether verbal, in writing or by way of trials - are given in good faith but without warranty, and this also applies where proprietary rights of third parties are involved. Our advice does not release you from the obligation to check its validity and to test our products as to their suitability for the intended processes and uses. The application, use and processing of our products and the products manufactured by you on the basis of our technical advice are beyond our control and, therefore, entirely your own responsibility. Our products are sold in accordance with our General Conditions of Sale and Delivery. The values stored in the databank should only be used as guidelines for component design. In giving these values neither guarantee, nor assurance of particular material properties can be given. techcenter.lanxess.com
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012