  Elastollan® S 95 A | TPU | BASF Polyurethanes GmbH
Описание продукта
DESCRIPTION
Elastollan S 95 A is a polyester based TPU

SPECIAL PROPERTIES
good wear performance, good damping behavior and rebound elasticity,
high tensile strength, good resistance to tear propagation

TYPICAL APPLICATIONS
sports shoe soles, roller tyres for conveyor systems and
shopping trolleys

OTHER HINTS
predrying: 2-3h at 100-110°C
(air circulating oven or dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
Теплофизические свойстваЗначениеЕдиницаСтандарт
Температура стеклования, 10°C/мин -24 °C ISO 11357-1/-2
Электрические свойстваЗначениеЕдиницаСтандарт
Сравнительный показатель пробоя 600 - IEC 60112
Прочие свойстваЗначениеЕдиницаСтандарт
Плотность 1240 кг/м³ ISO 1183
Параметры изготовления образцов для испытанийЗначениеЕдиницаСтандарт
Литье под давлением, температура расплава 220 °C ISO 294
Литье под давлением, температура пресс-формы 60 °C ISO 10724
Диаграммы
Динам. модуль упругости при сдвиге - температура , Elastollan® S 95 A, TPU, BASF PU
Напряжение - удлинение (ТЭП) , Elastollan® S 95 A, TPU, BASF PU
Особые свойства и характеристики
Способы переработки
Литье под давлением
Вид поставки
Гранулы
Доступность материала по регионам
Дискламация
The data contained in this publication are based on
our current knowledge and experience. In view of
the many factors that may affect processing and
application of our product, these data do not relieve
processors from carrying out their own investigations
and tests.  Any descriptions, drawings, photographs,
data, proportions, weights etc. given herein may
change without prior information and do not constitute
the agreed contractual quality of the product. It is
the responsibility of the recipient  of our products
to ensure that any proprietary rights and existing
laws and legislation are observed. NO WARRANTIES
OF ANY KIND, EITHER EXPRESS OR IMPLIED,
INCLUDING WARRANTIES OFMERCHANTABILITY OR
FITNESS FOR A PARTICULAR PURPOSE, ARE MADE
REGARDING PRODUCTS DESCRIBED OR DESIGNS,
DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY
BE USED WITHOUT INFRINGING THEINTELLECTUAL
PROPERTY RIGHTS OF OTHERS.

In order to check the availability of products please
contact us or our sales agency.


For more information about our products contact your
local BASF representative or

    BASF Polyurethanes GmbH
    European Business Management
    Thermoplastische Polyurethane
    Elastogranstraße 60
    D-49448 Lemförde
    Deutschland
    Telefon ++49 5443 122500
    Telefax ++49 5443 122555
    e-mail: pu-elastomere@basf.com
    www.pu.basf.de 
CAMPUS® is a registered trademark of CWFG (Chemie Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt) 

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012