  POLYMAN® (ABS) LP 137 A | ABS | A. Schulman GmbH
Описание продукта
Impact ABS grade with antistatic


Реологические свойстваЗначениеЕдиницаСтандарт
Показатель текучести расплава, ПТР 22 см³/10мин ISO 1133
Температура 220 °C ISO 1133
Нагрузка 10 кг ISO 1133
Механические свойстваЗначениеЕдиницаСтандарт
Модуль упругости при растяжении 2200 МПа ISO 527-1/-2
Напряжение в точке текучести 48 МПа ISO 527-1/-2
Удлинение в точке текучести 2.3 % ISO 527-1/-2
Ударная вязкость по Шарпи, +23°C N кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи с надрезом, +23°C 18 кДж/м2 ISO 179/1eA
Теплофизические свойстваЗначениеЕдиницаСтандарт
Температура размягчения по Вика, 50°C/ч 50Н 96 °C ISO 306
Класс горючести при номинальной толщине 1.5 мм HB класс IEC 60695-11-10
Толщина образца 1.5 мм IEC 60695-11-10
Соответствует стандарту UL - -
Электрические свойстваЗначениеЕдиницаСтандарт
Удельное объемное сопротивление >1E13 Ом*м IEC 60093
Удельное поверхностное сопротивление >1E15 Ом IEC 60093
Прочие свойстваЗначениеЕдиницаСтандарт
Плотность 1050 кг/м³ ISO 1183
Диаграммы
Удельный объем - Температура (pvT) , POLYMAN® (ABS) LP 137 A, ABS, A. Schulman
Особые свойства и характеристики
Способы переработки
Литье под давлением
Вид поставки
Мелкие гранулы
Особые показатели
Антистатический
Доступность материала по регионам
Дискламация
The information and recommendations contained in this document are based upon
data collected by A. Schulman and are believed to be reliable; however, because
A. Schulman cannot anticipate or control the many different conditions under
which this information and/or product may be used, no representation is made
and no warranty is given of any kind, express or implied, for completeness,
accuracy, availability, suitability, usefulness, commercial value, or non-violation
of intellectual property rights of information, recommendations, and products
and services directly or indirectly provided. A. Schulman assumes no responsibility
for the results of the use of products and processes described herein and expressly
disclaims the implied warranties of merchantability and fitness for a particular use

If there are questions to given information, to further properties or further A. Schulman
products please contact

                  A. Schulman GmbH
                  Huettenstrasse 211
                  50170 Kerpen
                  Tel: 02273 / 561-0
                  Contact: aschulman@de.aschulman.com
                               Subject: Material data

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012