- All Evonik Industries grades
- All PBT grades
- All grades beginning with V
CAMPUS® datasheet | VESTODUR® X7095 nc (nf)
This datasheet of VESTODUR® X7095 nc (nf) from Evonik Industries AG is provided by the international plastics database CAMPUS.
Resin: ISO 7792-PBT,MHR, A10-07,M30
VESTODUR® X7095 is a glass fiber reinforced semicrystalline thermoplastic resin for injection molding, based on
polybutylene terephthalate (PBT) with low warpage at parts made of this resin. The compound is suitable for the
manufacture of parts, which are subjected to high mechanical and thermal load.
| Реологические свойства | Значение | Единица | Стандарт |
| Показатель текучести расплава, ПТР | 12 | см³/10мин | ISO 1133 |
| Температура | 250 | °C | ISO 1133 |
| Нагрузка | 2.16 | кг | ISO 1133 |
| Усадка при литье, продольная | 0.5 | % | ISO 294-4, 2577 |
| Усадка при литье, поперечная | 1.8 | % | ISO 294-4, 2577 |
| Механические свойства | Значение | Единица | Стандарт |
| Модуль упругости при растяжении | 7000 | МПа | ISO 527-1/-2 |
| Напряжение при разрыве | 105 | МПа | ISO 527-1/-2 |
| Удлинение при разрыве | 4 | % | ISO 527-1/-2 |
| Ударная вязкость по Шарпи, +23°C | 30 | кДж/м2 | ISO 179/1eU |
| Ударная вязкость по Шарпи, -30°C | 30 | кДж/м2 | ISO 179/1eU |
| Ударная вязкость по Шарпи с надрезом, +23°C | 5.5 | кДж/м2 | ISO 179/1eA |
| Ударная вязкость по Шарпи с надрезом, -30°C | 4.5 | кДж/м2 | ISO 179/1eA |
| Теплофизические свойства | Значение | Единица | Стандарт |
| Температура плавления, 10°C/мин | 223 | °C | ISO 11357-1/-3 |
| Температура стеклования, 10°C/мин | 45 | °C | ISO 11357-1/-2 |
| Температура изгиба под нагрузкой, 1.80 МПа | 195 | °C | ISO 75-1/-2 |
| Температура изгиба под нагрузкой, 0.45 МПа | 220 | °C | ISO 75-1/-2 |
| Температура размягчения по Вика, 50°C/ч 50Н | 210 | °C | ISO 306 |
| Коэффициент линейного теплового расширения, продольный | 60 | E-6/K | ISO 11359-1/-2 |
| Коэффициент линейного теплового расширения, поперечный | 70 | E-6/K | ISO 11359-1/-2 |
| Класс горючести при номинальной толщине 1.5 мм | HB | класс | IEC 60695-11-10 |
| Толщина образца | 1.6 | мм | IEC 60695-11-10 |
| Класс горючести при толщине образца h | HB | класс | IEC 60695-11-10 |
| Толщина образца | 0.8 | мм | IEC 60695-11-10 |
| Электрические свойства | Значение | Единица | Стандарт |
| Относительная диэлектрическая проницаемость, 100Гц | 4 | - | IEC 60250 |
| Удельное объемное сопротивление | 1E13 | Ом*м | IEC 60093 |
| Удельное поверхностное сопротивление | 1E14 | Ом | IEC 60093 |
| Электрическая прочность | 27 | кВ/мм | IEC 60243-1 |
| Сравнительный показатель пробоя | 275 | - | IEC 60112 |
| Прочие свойства | Значение | Единица | Стандарт |
| Водопоглощение | 0.5 | % | Sim. to ISO 62 |
| Плотность | 1530 | кг/м³ | ISO 1183 |
| Параметры изготовления образцов для испытаний | Значение | Единица | Стандарт |
| Параметры процесса переработки согласно ISO | 7790 | - | ISO ....-2 |
| Литье под давлением, температура расплава | 260 | °C | ISO 294 |
| Литье под давлением, температура пресс-формы | 80 | °C | ISO 10724 |
| Литье под давлением, скорость впрыска | 200 | мм/с | ISO 294 |
| Литье под давлением, давление на стадии выдержки | 70 | МПа | ISO 294 |
All listed technical data are typical values intended for your guidance.
They are given without obligation and do not constitute a materials
specification. Should you have any further questions concerning material
behavior or properties, please contact us at the following address :
for PA: Evonik Industries AG
PP-HP-CRM
Gebäude 1227 / PB 16
D-45764 Marl
Phone: +49-(0)2365/49-2720
Fax:+49-(0)2365/49-2070
E-Mail: campusplastics@evonik.com
for PMMA: Evonik Industries AG
Marketing / Campus
Kirschenallee
D-64293 Darmstadt
Germany
Phone: +49 - (0) 61 51 / 18-47 11
Fax: +49 - (0) 61 51 / 18-31 77
E-Mail: campusplastics@evonik.com
Internet: http://www.plexiglas-polymers.com
® = registered trademark
PLEXIGLAS® is a registered trademark of Evonik Röhm GmbH, Germany,
outside of the Americas. Within the Americas it is sold as ACRYLITE®,
which is a registered trademark of Evonik Cyro LLC, USA.
PLEXIMID® is a registered trademarks of Evonik Röhm GmbH, Germany.
CYROLITE® and XT® polymer are registered trademarks of Evonik Cyro LLC, USA.
This information and all further technical advice is based on our present knowledge
and experience. However, it implies no liability or other legal responsibility on our part,
including with regard to existing third party intellectual property rights, especially
patent rights. In particular, no warranty, whether express or implied, or guarantee of
product properties in the legal sense is intended or implied. We reserve the right to
make any changes according to technological progress or further developments. The
customer is not released from the obligation to conduct careful inspection and testing
of incoming goods. Performance of the product described herein should be verified by
testing, which should be carried out only by qualified experts in the sole responsibility
of a customer. Reference to trade names used by other companies is neither a
recommendation, nor does it imply that similar products could not be used.
NAFTA:
This information and all technical and other advice are based on Evonik’s
present knowledge and experience. However, Evonik assumes no liability for
such information or advice, including the extent to which such information or
advice may relate to third party intellectual property rights. Evonik reserves the
right to make any changes to information or advice at any time, without prior
or subsequent notice. EVONIK DISCLAIMS ALL REPRESENTATIONS AND
WARRANTIES, WHETHER EXPRESS OR IMPLIED, AND SHALL HAVE NO LIABILITY
FOR, MERCHANTABILITY OF THE PRODUCT OR ITS FITNESS FOR A PARTICULAR
PURPOSE (EVEN IF EVONIK IS AWARE OF SUCH PURPOSE), OR OTHERWISE.
EVONIK SHALL NOT BE RESPONSIBLE FOR CONSEQUENTIAL, INDIRECT OR
INCIDENTAL DAMAGES (INCLUDING LOSS OF PROFITS) OF ANY KIND. It is the
customer’s sole responsibility to arrange for inspection and testing of all
products by qualified experts. Reference to trade names used by other
companies is neither a recommendation nor an endorsement of the
corresponding product, and does not imply that similar products could not be
used.
Sales range and technical data subject to alteration.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012