View list of

CAMPUS® datasheet | ALCOM® PBT 700/30.2 TCD2


This datasheet of ALCOM® PBT 700/30.2 TCD2 from ALBIS Plastic GmbH is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

  ALCOM® PBT 700/30.2 TCD2 | PBT... | ALBIS Plastic GmbH
机械性能价值单位测试标准
拉伸模量 8900 MPa ISO 527-1/-2
断裂应力 45 MPa ISO 527-1/-2
断裂伸长率 1.5 % ISO 527-1/-2
无缺口简支梁冲击强度, +23°C 30 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 4 kJ/m² ISO 179/1eA
热性能价值单位测试标准
热变形温度, 1.80 MPa 153 °C ISO 75-1/-2
维卡软化温度, 50°C/h 50N 200 °C ISO 306
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 3.2 mm IEC 60695-11-10
电性能价值单位测试标准
表面电阻率 1E12 Ohm IEC 60093
其它性能价值单位测试标准
密度 2470 kg/m³ ISO 1183
典型数据
加工方法
注塑
特殊性能
提高导电性, 经热稳处理的/耐热的
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012