机械性能价值单位测试标准
100%应变时的应力 3.2 MPa ISO 527-1/-2
断裂应变 TPE >300 % ISO 527-1/-2
时恒定应变下的永久变形, 100°C 37 % ISO 815
撕裂强度 33 kN/m ISO 34-1
肖氏硬度A, 3s 70 - ISO 868
其它性能价值单位测试标准
密度 970 kg/m³ ISO 1183
典型数据
加工方法
注塑, 其它挤出成型
特殊性能
经耐紫外线处理的/耐气候的
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012