CAMPUS® datasheet | ALTECH PA66 A 4040/100 MR40
This datasheet of ALTECH PA66 A 4040/100 MR40 from ALBIS Plastic GmbH is provided by the international plastics database CAMPUS.
You may contact the supplier for more information about this grade.
ALTECH PA66 A 4040/100 MR40 | PA66-MX40 | ALBIS Plastic GmbH
| 机械性能 | 干 / 已调节 | 单位 | 测试标准 |
| 拉伸模量 | 6500 / 4500 | MPa | ISO 527-1/-2 |
| 断裂应力 | 90 / 75 | MPa | ISO 527-1/-2 |
| 断裂伸长率 | 6 / 15 | % | ISO 527-1/-2 |
| 无缺口简支梁冲击强度, +23°C | 80 / - | kJ/m² | ISO 179/1eU |
| 简支梁缺口冲击强度, +23°C | 4 / - | kJ/m² | ISO 179/1eA |
| 热性能 | 干 / 已调节 | 单位 | 测试标准 |
| 熔融温度, 10°C/min | 253 / * | °C | ISO 11357-1/-3 |
| 热变形温度, 1.80 MPa | 120 / * | °C | ISO 75-1/-2 |
| 热变形温度, 0.45 MPa | 235 / * | °C | ISO 75-1/-2 |
| 维卡软化温度, 50°C/h 50N | 200 / * | °C | ISO 306 |
权利义务的法律声明
Any information given on the chemical and physical characteristics of our products, including technical advice on applications whether verbally, in writing or by testing the product, is given to the best of our knowledge, but without warranty. It does not exempt the buyer from carrying out his own investigations and tests in order to ascertain the products' specific suitability for the purpose intended. The buyer is solely responsible for the application, utilisation and processing of the products, and must observe the laws and government regulations and the consequential rights of any third party. At all times our Conditions of Sale apply. The test values given are guide values, not binding minimum or maximum figures, which have been determined on standardized test specimen and can be affected by pigmentation, mold design and processing conditions.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012