  ALTECH PC C 1000/100 | PC | ALBIS Plastic GmbH
流变性能价值单位测试标准
熔体体积流动速度, MVR 11 cm³/10min ISO 1133
温度 300 °C ISO 1133
载荷 1.2 kg ISO 1133
机械性能价值单位测试标准
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 10 kJ/m² ISO 179/1eA
热性能价值单位测试标准
维卡软化温度, 50°C/h 50N 141 °C ISO 306
电性能价值单位测试标准
体积电阻率 1E11 Ohm*m IEC 60093
其它性能价值单位测试标准
密度 1200 kg/m³ ISO 1183
典型数据
加工方法
注塑
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012