  ALTECH PP-H A 1000/149 FR | PP FR | ALBIS Plastic GmbH
流变性能价值单位测试标准
熔体体积流动速度, MVR 6 cm³/10min ISO 1133
温度 230 °C ISO 1133
载荷 2.16 kg ISO 1133
机械性能价值单位测试标准
拉伸模量 1300 MPa ISO 527-1/-2
无缺口简支梁冲击强度, +23°C 80 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 4 kJ/m² ISO 179/1eA
热性能价值单位测试标准
熔融温度, 10°C/min 163 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 54 °C ISO 75-1/-2
热变形温度, 0.45 MPa 85 °C ISO 75-1/-2
维卡软化温度, 50°C/h 50N 85 °C ISO 306
1.5mm名义厚度时的燃烧性 V-2 class IEC 60695-11-10
测试用试样的厚度 1.5 mm IEC 60695-11-10
电性能价值单位测试标准
体积电阻率 >1E13 Ohm*m IEC 60093
表面电阻率 1E13 Ohm IEC 60093
其它性能价值单位测试标准
密度 950 kg/m³ ISO 1183
典型数据
加工方法
注塑
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012