View list of
CAMPUS® datasheet | Elastollan® C 85 A HPM
This datasheet of Elastollan® C 85 A HPM from BASF Polyurethanes GmbH is provided by the international plastics database CAMPUS.
You may contact the supplier for more information about this grade.
Elastollan® C 85 A HPM | TPU | BASF Polyurethanes GmbH
材料文字说明
DESCRIPTION
Elastollan C 85 A HPM is a polyester based TPU
SPECIAL PROPERTIES
high tensile strength, excellent tear strength,
very good damping behavior, good rebound elasticity,
very good wear performance, good flexibility at low temperature and
resistance to hydrolysis, improved heat distortion temperature
TYPICAL APPLICATIONS
technical parts
OTHER HINTS
predrying: 2-3h at ca. 85°C (dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties
CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
Elastollan C 85 A HPM is a polyester based TPU
SPECIAL PROPERTIES
high tensile strength, excellent tear strength,
very good damping behavior, good rebound elasticity,
very good wear performance, good flexibility at low temperature and
resistance to hydrolysis, improved heat distortion temperature
TYPICAL APPLICATIONS
technical parts
OTHER HINTS
predrying: 2-3h at ca. 85°C (dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties
CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
| 机械性能 | 价值 | 单位 | 测试标准 |
| 100%应变时的应力 | 6 | MPa | ISO 527-1/-2 |
| 300%应变时的应力 | 11 | MPa | ISO 527-1/-2 |
| 断裂应力 TPE | 50 | MPa | ISO 527-1/-2 |
| 断裂应变 TPE | >300 | % | ISO 527-1/-2 |
| 时恒定应变下的永久变形, 23°C | 15 | % | ISO 815 |
| 时恒定应变下的永久变形, 70°C | 25 | % | ISO 815 |
| 撕裂强度 | 70 | kN/m | ISO 34-1 |
| 耐磨性 | 35 | mm³ | ISO 4649 |
| 肖氏硬度A, 3s | 85 | - | ISO 868 |
| 其它性能 | 价值 | 单位 | 测试标准 |
| 密度 | 1230 | kg/m³ | ISO 1183 |
函数
权利义务的法律声明
The data contained in this publication are based on
our current knowledge and experience. In view of
the many factors that may affect processing and
application of our product, these data do not relieve
processors from carrying out their own investigations
and tests. Any descriptions, drawings, photographs,
data, proportions, weights etc. given herein may
change without prior information and do not constitute
the agreed contractual quality of the product. It is
the responsibility of the recipient of our products
to ensure that any proprietary rights and existing
laws and legislation are observed. NO WARRANTIES
OF ANY KIND, EITHER EXPRESS OR IMPLIED,
INCLUDING WARRANTIES OFMERCHANTABILITY OR
FITNESS FOR A PARTICULAR PURPOSE, ARE MADE
REGARDING PRODUCTS DESCRIBED OR DESIGNS,
DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY
BE USED WITHOUT INFRINGING THEINTELLECTUAL
PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please
contact us or our sales agency.
For more information about our products contact your
local BASF representative or
BASF Polyurethanes GmbH
European Business Management
Thermoplastische Polyurethane
Elastogranstraße 60
D-49448 Lemförde
Deutschland
Telefon ++49 5443 122500
Telefax ++49 5443 122555
e-mail: pu-elastomere@basf.com
www.pu.basf.de CAMPUS® is a registered trademark of CWFG (Chemie Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012