  Grivory HT2VZ-33H black 9205 | PA6T/66-GF33 | EMS-GRIVORY - a unit of EMS-CHEMIE AG
材料文字说明
Product designation according to ISO 1874:

PA 6T/66, MH, 14-110, GF33

 

Product Attributes

  Improved impact resistance, Improved heat resistance, Improved UV resistance (outdoor use)

Markets

  Automotive
  Automotive electr. and electronics, lighting, Fuel systems, Powertrain and Chassis , Interior,
Exterior
  Electricals & Electronics
  Electrical equipment, Connectors
  Industry & Consumer goods
  Housewares, Hydraulics & Pneumatics, Mechanical Engineering, Power transmission, Sports & Leisure,
Tools & Accessories
流变性能干 / 已调节单位测试标准
模塑收缩率, 平行 0.1 / * % ISO 294-4, 2577
模塑收缩率, 垂直 0.9 / * % ISO 294-4, 2577
机械性能干 / 已调节单位测试标准
拉伸模量 11000 / 11000 MPa ISO 527-1/-2
断裂应力 200 / 180 MPa ISO 527-1/-2
断裂伸长率 2.5 / 2.5 % ISO 527-1/-2
无缺口简支梁冲击强度, +23°C 55 / 55 kJ/m² ISO 179/1eU
无缺口简支梁冲击强度, -30°C 50 / 45 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 10 / 10 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 9 / 9 kJ/m² ISO 179/1eA
热性能干 / 已调节单位测试标准
熔融温度, 10°C/min 310 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 285 / * °C ISO 75-1/-2
热变形温度, 8.00 MPa 200 / * °C ISO 75-1/-2
线性热膨胀系数, 平行 20 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 60 / * E-6/K ISO 11359-1/-2
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 0.8 / * mm IEC 60695-11-10
电性能干 / 已调节单位测试标准
体积电阻率 1E10 / 1E10 Ohm*m IEC 60093
表面电阻率 * / 1E12 Ohm IEC 60093
介电强度 38 / 37 kV/mm IEC 60243-1
相对漏电起痕指数 - / 600 - IEC 60112
其它性能干 / 已调节单位测试标准
吸水性 5 / * % 类似ISO 62
吸湿性 2 / * % 类似ISO 62
密度 1440 / - kg/m³ ISO 1183
典型数据
加工方法
注塑
供货形式
粒料
特殊性能
经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
地区供应
权利义务的法律声明
EMS-CHEMIE AG
Business Unit EMS-GRIVORY

Homepage : EMS-GRIVORY
eMail    : welcome@emsgrivory.com


The values are intended to serve as an aid in preselecting materials and for
an overview of the EMS-GRIVORY product  range. The information contained
in this publication is based on our present knowledge and experience.
The given figures and data are guidance values and do not represent binding
material specifications. No warranties of any kind, either express or implied,
including warranties of merchantability or fitness for a particular purpose, are
given regarding products, design, data and information. The customer is not
released from his obligation to investigate the products fitness and the suitability
for the intended application, compliance with legal requirements and intellectual
property rights. We reserve the right to change the information at any time and
without prior notice. The information in this publication is not to be considered
a contractual obligation and any liability whatsoever is expressly declined.
For further questions about our products please contact our experts.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012