View list of
  • All ARKEMA grades
  • All PVDF grades
  • All grades beginning with K

CAMPUS® datasheet | Kynar® FLEX 3120-50


This datasheet of Kynar® FLEX 3120-50 from ARKEMA is provided by the international plastics database CAMPUS.

This datasheet includes:

  Kynar® FLEX 3120-50 | PVDF | ARKEMA
材料文字说明
 

Kynar® FLEX 3120-50

 

 

Kynar® FLEX are fluorinated thermoplastic copolymers.

 

Outstanding characteristics of Kynar® FLEX : chemical resistance,

imperviousness to UV, high barrier properties, high purity,good mechanical

and thermomechanical properties.

 

Main applications of Kynar® FLEX : corrosion protection in the chemical

industry, coating (painting, extrusion), wire and cable.

 

Kynar® FLEX 3120-50 is a grade which exhibits, compared to 2800,

a higher melting point which allows a greater range for use.

For cable coating, extrusion of tube and plaque, compression moulding

of bulky parts.

流变性能价值单位测试标准
熔体体积流动速度, MVR 0.5 cm³/10min ISO 1133
温度 230 °C ISO 1133
载荷 5 kg ISO 1133
机械性能价值单位测试标准
拉伸模量 690 MPa ISO 527-1/-2
屈服应力 28 MPa ISO 527-1/-2
屈服伸长率 12 % ISO 527-1/-2
名义断裂伸长率 >50 % ISO 527-1/-2
热性能价值单位测试标准
熔融温度, 10°C/min 165 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min -46 °C ISO 11357-1/-2
其它性能价值单位测试标准
密度 1780 kg/m³ ISO 1183
试样制备条件价值单位测试标准
压缩, 模具温度 225 °C ISO 293
压缩, 保压时间 3 min ISO 293
压缩, 脱模温度 120 °C ISO 293
典型数据
加工方法
异型材挤出成型, 其它挤出成型
供货形式
粒料
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
地区供应
权利义务的法律声明
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed