ABS-PC blend with increased impact strength, heat resistance and good flow behaviour


流变性能价值单位测试标准
熔体体积流动速度, MVR 16 cm³/10min ISO 1133
温度 260 °C ISO 1133
载荷 5 kg ISO 1133
模塑收缩率, 平行 0.4 % ISO 294-4, 2577
模塑收缩率, 垂直 0.4 % ISO 294-4, 2577
机械性能价值单位测试标准
拉伸模量 2300 MPa ISO 527-1/-2
屈服应力 49 MPa ISO 527-1/-2
屈服伸长率 4 % ISO 527-1/-2
名义断裂伸长率 39 % ISO 527-1/-2
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
无缺口简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 39 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 17 kJ/m² ISO 179/1eA
热性能价值单位测试标准
玻璃化转变温度, 10°C/min 141 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 99 °C ISO 75-1/-2
热变形温度, 0.45 MPa 105 °C ISO 75-1/-2
维卡软化温度, 50°C/h 50N 115 °C ISO 306
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm IEC 60695-11-10
UL注册 UL - -
电性能价值单位测试标准
体积电阻率 >1E13 Ohm*m IEC 60093
表面电阻率 >1E15 Ohm IEC 60093
其它性能价值单位测试标准
密度 1110 kg/m³ ISO 1183
流变计算用参数价值单位测试标准
熔体密度 980 kg/m³ -
熔体 0.2 W/(m K) -
有效导热率a 9.3E-8 m²/s -
喷射温度 115 °C -
试样制备条件价值单位测试标准
ISO试样制备条件. 2580 - ISO ....-2
注塑, 熔体温度 250 °C ISO 294
注塑, 模具温度 60 °C ISO 10724
注塑, 注射速度 250 mm/s ISO 294
注塑, 保压压力 100 MPa ISO 294
典型数据
加工方法
注塑
供货形式
碎粒料
添加剂
脱模助剂
特殊性能
可电镀的
地区供应
权利义务的法律声明
The information and recommendations contained in this document are based upon
data collected by A. Schulman and are believed to be reliable; however, because
A. Schulman cannot anticipate or control the many different conditions under
which this information and/or product may be used, no representation is made
and no warranty is given of any kind, express or implied, for completeness,
accuracy, availability, suitability, usefulness, commercial value, or non-violation
of intellectual property rights of information, recommendations, and products
and services directly or indirectly provided. A. Schulman assumes no responsibility
for the results of the use of products and processes described herein and expressly
disclaims the implied warranties of merchantability and fitness for a particular use

If there are questions to given information, to further properties or further A. Schulman
products please contact

                  A. Schulman GmbH
                  Huettenstrasse 211
                  50170 Kerpen
                  Tel: 02273 / 561-0
                  Contact: aschulman@de.aschulman.com
                               Subject: Material data

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012