View list of
- All A. Schulman grades
- All PBT grades
- All grades beginning with S
CAMPUS® datasheet | SCHULADUR® A GF 10
This datasheet of SCHULADUR® A GF 10 from A. Schulman GmbH is provided by the international plastics database CAMPUS.
You may contact the supplier for more information about this grade.
SCHULADUR® A GF 10 | PBT-GF10 | A. Schulman GmbH
材料文字说明
10% glass fibre reinforced PBT
| 流变性能 | 价值 | 单位 | 测试标准 |
| 熔体体积流动速度, MVR | 30 | cm³/10min | ISO 1133 |
| 温度 | 250 | °C | ISO 1133 |
| 载荷 | 2.16 | kg | ISO 1133 |
| 机械性能 | 价值 | 单位 | 测试标准 |
| 拉伸模量 | 4500 | MPa | ISO 527-1/-2 |
| 断裂应力 | 90 | MPa | ISO 527-1/-2 |
| 断裂伸长率 | 3.5 | % | ISO 527-1/-2 |
| 无缺口简支梁冲击强度, +23°C | 19 | kJ/m² | ISO 179/1eU |
| 简支梁缺口冲击强度, +23°C | 5 | kJ/m² | ISO 179/1eA |
| 热性能 | 价值 | 单位 | 测试标准 |
| 熔融温度, 10°C/min | 230 | °C | ISO 11357-1/-3 |
| 玻璃化转变温度, 10°C/min | 22 | °C | ISO 11357-1/-2 |
| 热变形温度, 1.80 MPa | 185 | °C | ISO 75-1/-2 |
| 热变形温度, 0.45 MPa | 215 | °C | ISO 75-1/-2 |
| 1.5mm名义厚度时的燃烧性 | HB | class | IEC 60695-11-10 |
| 测试用试样的厚度 | 1.6 | mm | IEC 60695-11-10 |
| 流变计算用参数 | 价值 | 单位 | 测试标准 |
| 熔体密度 | 1050 | kg/m³ | - |
| 试样制备条件 | 价值 | 单位 | 测试标准 |
| ISO试样制备条件. | 7790 | - | ISO ....-2 |
| 注塑, 熔体温度 | 260 | °C | ISO 294 |
| 注塑, 模具温度 | 80 | °C | ISO 10724 |
| 注塑, 注射速度 | 250 | mm/s | ISO 294 |
| 注塑, 保压压力 | 70 | MPa | ISO 294 |
权利义务的法律声明
The information and recommendations contained in this document are based upon
data collected by A. Schulman and are believed to be reliable; however, because
A. Schulman cannot anticipate or control the many different conditions under
which this information and/or product may be used, no representation is made
and no warranty is given of any kind, express or implied, for completeness,
accuracy, availability, suitability, usefulness, commercial value, or non-violation
of intellectual property rights of information, recommendations, and products
and services directly or indirectly provided. A. Schulman assumes no responsibility
for the results of the use of products and processes described herein and expressly
disclaims the implied warranties of merchantability and fitness for a particular use
If there are questions to given information, to further properties or further A. Schulman
products please contact
A. Schulman GmbH
Huettenstrasse 211
50170 Kerpen
Tel: 02273 / 561-0
Contact: aschulman@de.aschulman.com
Subject: Material data
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012